TECHNET Archives

January 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Stadem, Richard D." <[log in to unmask]>
Date:
Thu, 26 Jan 2006 10:12:26 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Jeffrey Bush <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
Jeffrey Bush <[log in to unmask]>
Parts/Attachments:
text/plain (87 lines)
Direct Immersion Gold (DIG) is also a finish that should be looked at as
it is developed.  The initial look that we have taken looks good and I
think this finish may be a good alternative in the near future.  

I know George is listening and he has some good information on the
technology.

Jeffrey Bush
Director, Quality Assurance and Technical Support
VERMONT CIRCUITS INCORPORATED 
           76 Technology Drive - POB 1890 
              Brattleboro, Vermont 05302
                Voice - 802.257.4571 ext 37 
                    Fax - 802.257.0011
                       <http://www.vtcircuits.com/> 
                           
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
Sent: Thursday, January 26, 2006 8:24 AM
To: [log in to unmask]
Subject: Re: [TN] Immersion Gold and LF PROCESS

Well, immersion silver is still cheaper than gold over nickel.
The cheapest alternative is OSP, but I would not recommend it. It
depends also on the type of assembly and its application.
Immersion tin may be an alternative, but I would not recommend that
either, as it has serious storage and long-term reliability issues.  

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of [log in to unmask]
Sent: Wednesday, January 25, 2006 7:38 PM
To: [log in to unmask]
Subject: Re: [TN] Immersion Gold and LF PROCESS

Richard:  Thanks so much for the help.....much appreciated!!!!   My boss
is
now askiing me to look in other directions vs. SAC305, with the price
of silver skyrocketing.  Any suggestions?
As a contract manufacturer, we see a huge variety of applications, so I
am reluctant to go into something that the rest of the world has not
fully investigated.

Thanks for your help!!!!!

Best regards,
Bill

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2