It could also be a case that something in the potting compound is
inhibiting the cure reaction, allowing bubbles to form later in urethane
that is not fully cured. If the potting compound is not completely cured,
there could be some chemical critters running around causing havoc. Are
you thinning the urethane to spray? Got any pictures that Steve could put
on his web page to look at?
Doug Pauls
Phil Nutting
<PNutting@KAISERS
YSTEMS.COM> To
Sent by: TechNet [log in to unmask]
<[log in to unmask]> cc
Subject
01/24/2006 09:29 Re: [TN] Conforma Coat (Urethane) &
AM bubbles
Please respond to
TechNet E-Mail
Forum
<[log in to unmask]>
; Please respond
to
Phil Nutting
<PNutting@KAISERS
YSTEMS.COM>
Kelly,
Sounds like either a chemical reaction or an air void that is working
its way to the surface during heat curing.
Phil Nutting
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Kelly Morris
Sent: Tuesday, January 24, 2006 10:25 AM
To: [log in to unmask]
Subject: [TN] Conforma Coat (Urethane) & bubbles
We've got a problem here, where we're hand spraying a urethane conformal
coat on over a rectangular inductor.
The inductor body is a plastic tube, with potting to fill.
The top is not always flat (sometimes concave).
The problem is that bubbles appear in the conformal coat on the potted
surface, sometimes right after bake and sometimes days after.
Any ideas on what the root cause is and how to prevent the bubbles?
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|