TECHNET Archives

January 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Kane, Amol (349)" <[log in to unmask]>
Date:
Wed, 18 Jan 2006 15:41:39 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Dehoyos, Ramon" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
"Dehoyos, Ramon" <[log in to unmask]>
Parts/Attachments:
text/plain (192 lines)
                Yes, it will be eliminated at the solder area, due to
the fact that Sn is no longer pure, > 3% of other metals.   The concern
still exists at the terminal source where there is no solder of any
kind. Whiskers may still grow there and either short out with adjacent
terminals or break out and short leads by bridging them.
        Regards,
        Ramon
 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Kane, Amol (349)
Sent: Wednesday, January 18, 2006 2:54 PM
To: [log in to unmask]
Subject: Re: [TN] RoHS board finish

...on a related issue.....any thoughts about Sn whiskering propensity of
Immersion Sn finish? My knowledge base seems to tell me that Immersion
Sn is popular in Europe and to date has no evidence (published) of tin
whiskering due to the finish....another train of though is that if you
solder the surface that's coated with Immersion Sn, then the whiskering
propensity (if any) of Immersion Sn finish is eliminated

Any thoughts???

Amol Kane
M.S (Industrial Eng.)
Process Engineer
Harvard Custom Manufacturing
941 Route 38  Owego, NY 13827
Phone: (607) 687-7669 x349
[log in to unmask]

 -----Original Message-----
From:   TechNet [mailto:[log in to unmask]]  On Behalf Of Kane, Amol (349)
Sent:   Wednesday, January 18, 2006 2:49 PM
To:     [log in to unmask]
Subject:        Re: [TN] RoHS board finish

Hi,
We are experimenting with Immersion Ag and Sn......and so far both of
these finishes seem to be at par in terms of solderability, and time
zero shear and pull testing results. Accelerated thermal cycling is
being performed to see long term reliability.

Amol Kane
M.S (Industrial Eng.)
Process Engineer
Harvard Custom Manufacturing
941 Route 38  Owego, NY 13827
Phone: (607) 687-7669 x349
[log in to unmask]

 -----Original Message-----
From:   TechNet [mailto:[log in to unmask]]  On Behalf Of Stadem, Richard
D.
Sent:   Wednesday, January 18, 2006 2:26 PM
To:     [log in to unmask]
Subject:        Re: [TN] RoHS board finish

Good words, John. I like "bullet-proof". 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of John Burke
Sent: Wednesday, January 18, 2006 11:55 AM
To: [log in to unmask]
Subject: Re: [TN] RoHS board finish

Polyclad 370HR finished in immersion silver will be pretty much bullet
proof.

Kind regards,

John Burke

John

John Burke
Senior Manager - Operations , Optichron
[log in to unmask]
W: 510 249 5233
M: 408 515 4992
http://www.optichron.com
Profile: https://www.linkedin.com/e/fps/2665502/

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Robert Walker
Sent: Wednesday, January 18, 2006 9:39 AM
To: [log in to unmask]
Subject: [TN] RoHS board finish

Hi All,

I'm doing my first PCB design that will use lead-free components and I
need to change my board finish from what I've always used.....HASL. I'm
looking for  any recommendations or comments on the best board finish to
use.

The components used on the design will be a mixture of tin-lead and
lead-free (SAC), so I'm not sure if there is a preferred finish to use
in this  type of situation. I work in a prototype environment where the
boards may be reworked (BGA removal/replaced) a number of times, so I'm
concerned about the ability of the finish being able to handle being
reworked/reflowed a number of times.

I'd also welcome any recommendations on the type of board material to
use since it will see an elevated temperature of up to 260C. I've always
just specified FR4 in the past.

Thanx in advance for any feedback.

Regards,
Bob Walker
[log in to unmask] (mailto:[log in to unmask])

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2