Trevor Chainey <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Trevor Chainey <[log in to unmask]>
Date:
Mon, 19 Dec 2005 14:37:10 -0000
Content-Type:
text/plain
Parts/Attachments:
text/plain (64 lines)
I'll tell you anyway: Item 6 of the Annex to the Directive - exemptions to
article 4.

Trevor.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Tempea, Ioan
Sent: Monday, December 19, 2005 14:24
To: [log in to unmask]
Subject: Re: [TN] verifying RoHS Compliance

Trevor,

I will not ask where this information is, I have not studied the directives.
But it would be good to know the source, though ;o)

What I wonder is how will it be measured? In the assembler's incoming it
would be OK to scrape the plating off and put the part on the XRF, but once
we deal with finished product, it gets rather complicated.

Thanks,
Ioan

> -----Original Message-----
> From: TechNet [SMTP:[log in to unmask]] On Behalf Of Trevor Chainey
> Sent: Monday, December 19, 2005 9:06 AM
> To:   [log in to unmask]
> Subject:      Re: [TN] verifying RoHS Compliance
>
> Phil/Mike,
>
> Lead up to a maximum of 4.0% is permitted in copper alloy.
>
>
> Trevor Chainey
> Quality Manager
> Telesoft Technologies Ltd
> Telephone +44 (0)1258 486568
>
>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2