Is it possible to get an acceptable solder joint if a Pb free BGA is put onto a board using SnPb solder paste and normal SnPb
profiles?
The lead free solder balls are SnAgCu 96.5/3/0.5.
Seems nigh impossible to get DDR2 packages with SnPb balls.
I'm designing a high end DSP into an industrial instrument. The DSP is not available lead free, nor does the application call
for lead free (thankfully).
There is no option to use a different memory type with the DSP. Nor is there any possibility of using a different DSP or FPGA
due to time/cost/sanity.
Don't want to explore going lead free on this one (for obvious reasons), and certainly do not welcome the expense of reballing
0.8mm DDR2 chips.
Best Regards
David Greig
______________________________
GigaDyne Ltd
Buchan House
Carnegie Campus
Dunfermline KY11 8PL
United Kingdom
t: +44 (0)1383 624 975
www.gigadyne.co.uk <http://www.gigadyne.co.uk/>
______________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------