TECHNET Archives

December 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Dale Ritzen <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Dale Ritzen <[log in to unmask]>
Date:
Mon, 12 Dec 2005 08:07:44 -0600
Content-Type:
text/plain
Parts/Attachments:
text/plain (71 lines)
Chris,
Alternative #3: Just have the cast iron pot replaced. It might be almost as
expensive as buying a whole new unit, but might not be as well. The only
hang out here is the leaded solder inside the other parts of the machine.
How do you get THAT out?

Anyone else try this?

Dale Ritzen
Quality Manager
Austin Manufacturing Services

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Schaefer, Chris
Sent: Monday, December 12, 2005 7:58 AM
To: [log in to unmask]
Subject: Re: [TN] Preparing Solder Pot for Lead Free Processing


Thank you all.

So should I do one of the following:

- Replace the solder pot altogether (the safest method, but most expensive)
- Clean the existing cast iron pot as best possible then fill with Pb Free
solder (higher risk, but less expensive)

If anyone has cleaned their existing cast iron  solder pot, then how did you
do it exactly? Is there a proposed method for doing this somewhere out
there?

Any suggestions would be very helpful.

CAS

        -----Original Message-----
        From: [log in to unmask] [mailto:[log in to unmask]]
        Sent: Fri 12/9/2005 11:10 AM
        To: Schaefer, Chris; [log in to unmask]
        Cc:
        Subject: Re: [TN] Preparing Solder Pot for Lead Free Processing


        Hi Chris,
        Pb left in the old 'pot' may not be your biggest problem--look at
these pics.




        Regards,
        Werner Engelmaier
        Engelmaier Associates, L.C.
        Electronic Packaging, Interconnection and Reliability Consulting
        7 Jasmine Run
        Ormond Beach, FL 32174 USA
        Phone: 386-437-8747, Fax: 386-437-8737, Cell: 386-316-5904
        E-mail: [log in to unmask], Website: www.engelmaier.com



---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2