This is a strange question from a designer's point of view... If you send me
a board with "nonwetted or insufficient soldered pads" we will reject them.
100% of all solder locations must be properly soldered, all the time, every
day, no exceptions. There is no criteria for 'acceptable numbers' for bad
solder joints. The circuit will not work or be reliable unless they are all
good solder joints. You cannot tolerate bad solder or dewetted surface
finishes.
Now... if you are looking for statistical figures for the industry about how
much scrap or rework assembly houses make, someone else will have to answer
that one... Although it occurs to me that data might be a point of interest
to someone trying to set up or run a board shop and figure out the costs of
doing business...
Your company BaskiDevre is in the business of making boards is it not?... I
would expect that your Quality Assurance people would have collected this
statistic and it would be used as a running gauge for seeing if they had
control of their processes and were maintaining them correctly in order to
keep those numbers as small as possible with the equipment and methods that
they had to work with. The ideal situation would be zero defects, like John
Burke says. That would mean your process controls were working.
Best regards,
Bill Brooks - KG6VVP
PCB Design Engineer, C.I.D.+, C.I.I.
Tel: (760)597-1500 Ext 3772 Fax: (760)597-1510
Datron World Communications, Inc.
_______________________________________
San Diego Chapter of the IPC Designers Council
Communications Officer, Web Manager
http://dcchapters.ipc.org/SanDiego/
http://pcbwizards.com
-----Original Message-----
From: Baski Devre [mailto:[log in to unmask]]
Sent: Monday, December 05, 2005 9:05 AM
To: [log in to unmask]
Subject: Re: [TN] Nonwetting Pad numbers
I may ask wrongly so please let me ask again. What is the ppm of
nonwetted or insufficient soldered pads numbers which will be touched up
after assembly of the PCBs
John Burke yazmış:
>That would be zero
>john
>Sent with Wireless Sync from Verizon Wireless
>
>---- Original Message ----
>From: "Baski Devre" <[log in to unmask]>
>Date: 12/5/05 8:42 am
>To: "[log in to unmask]" <[log in to unmask]>
>Subj: [TN] Nonwetting Pad numbers
>Dear Technetters
>What are the acceptibility criteria of nonwetting PCB for a PCB which
>has about thousand pads both smd pads and through hole pads.holes .
>Or, is there any standard which can state that after assembly how many
>pads are tolerant to not being soldered per 1,000 pads.
>Best Regards
>
>
>
--
Yusuf GÖMEÇ
Product Quality Engineer
BASKI DEVRE SAN ve TIC LTD STI
Ceyhan Sk. No:10 34896 Pendik-Istanbul-Turkey
Tel: 00 90 216 3901036 (4 Hat/Line)-173(Extention)
00 90 216 4836560 (4 Hat/Line)-173(Extention)
Fax: 00 90 216 3544941
00 90 216 4913269
Gsm: 00 90 533 6579897
00 90 533 7480014
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|