TECHNET Archives

December 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Alan Kreplick <[log in to unmask]>
Date:
Thu, 8 Dec 2005 12:05:08 +0100
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Ingemar Hernefjord <[log in to unmask]>
Subject:
From:
Ingemar Hernefjord <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (49 lines)
We use std profile. BGAs are allowed to reflow 5 times,  and overheating
has never been a problem. Deviations from std routines use to be
dubious.
 
Inge
 
-----Ursprungligt meddelande-----
Från: TechNet [mailto:[log in to unmask]] För Alan Kreplick
Skickat: den 7 december 2005 22:35
Till: [log in to unmask]
Ämne: [TN] BGA Rework Max temp & time above Liquidus
 

Hello Technetters: 

Quick survey/question: For BGA removal/replacement (SN63), what are
people using for max solder joint temperature and it's associated time
above liquidus. 

Copying the reflow profile guidelines?  I've previously went about 5-10C
less than the reflow profile guidelines to prevent overheating of the
part/case and to attempt to prevent any BGA's on the bottom-side from
re-reflowing, but now I'm second guessing myself. 

Thanks in advance.

 
Raytheon


Al Kreplick
Sr. Manufacturing Engineer
Land Combat/Precision Strike/Air to Air
978.470.9931
978.470.4307 fax
978-245-1702 pager
 <mailto:[log in to unmask]> [log in to unmask] 
 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2