I am looking for information regarding stencil design for fine-pitch
lead-free applications. I am interested to see what most people are doing
for the aperture size. Are you reducing or going 1 to 1? If you are reducing
what is the reduction formula? Are you reducing the same regardless of
aperture stance to print direction? Any input would be much appreciated.
Joel Mearig
Delta Tau Data Systems, Inc.