What type of component is it? Maybe it's RoHS exempt?
3% is about 30 times too high for all but exempt components, so check
and see if you have one of those exemptions.
If no exemption, then you should do what our CM does, and stop the
components in incoming inspection and notify your customer.
They are the ones responsible for the BOM, but if you let it pass, then
the responsibility could end up biting you.
asta.
Rick Smith
Senior Materials & Process Engineer
Phone: (512)652-3544
Fax: (512)652-3545
Cell: (512)299-6925
Email: [log in to unmask]
ClearCube Technology, Inc
8834 Capital of Texas Hwy N
Austin, TX 78759
www.clearcube.com
-----Original Message-----
From: Leadfree [mailto:[log in to unmask]] On Behalf Of Cagle, James
Sent: Wednesday, December 28, 2005 3:46 PM
To: [log in to unmask]
Subject: [LF] What is really leadfree
We have parts that are reading that have lead (over 1000ppm) that are
labeled lead-Free. We were told the parts are Homogenous and could
contain up to 3% lead and were RoHSCompliant. My question is what or
when is a part really leadfree?
We are a CM working from a customer's BOM so who is responsible?
------------------------------------------------------------------------
-------Leadfee Mail List provided as a service by IPC using LISTSERV
1.8d
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks
send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
------------------------------------------------------------------------
-------
-------------------------------------------------------------------------------Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-------------------------------------------------------------------------------
|
|
|