Another issue you have to consider is the ESD generated; it can
be in the thousands. Some ESD sensitive components can not take it. The
CCR1000 can be sprayed away from the BGA or the BGA can be water soluble
or peelable masked.
Regards,
Ramon
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Douglas O. Pauls
Sent: Monday, December 19, 2005 12:16 PM
To: [log in to unmask]
Subject: Re: [TN] senior chemist at HumiSeal
Sodium bicarbonate (Crystal Marks #34 powder) works well, but be careful
as it can be darned aggressive. You might consider their #25 powder,
which is a wheat starch base. A little slower, but does not damage mask
or part markings.
Doug Pauls
"Joseph H. Smith"
<agkettle@NETSCAP
E.NET>
To
Sent by: TechNet [log in to unmask]
<[log in to unmask]>
cc
Subject
12/19/2005 10:43 Re: [TN] senior chemist at
HumiSeal
AM
Please respond to
TechNet E-Mail
Forum
<[log in to unmask]>
; Please respond
to
agkettle@NETSCAPE
.NET
Ramon,
I have tried the 'bead blasting' method and I am very impressed with the
results. On my application, I still had some issues with removal of the
blasting media. Wash could not get all the beads out from under BGA's.
I have another source that uses Sodium BiCarbonate as the media. Claims
that it water soluable. Company is Crystal Mark in California.
Andrew Kettlewell
Sr Process Engineer
Sypris Electronics
Tampa, Fl
-----Original Message-----
From: Dehoyos, Ramon <[log in to unmask]>
To: [log in to unmask]
Sent: Fri, 16 Dec 2005 08:32:27 -0500
Subject: Re: [TN] senior chemist at HumiSeal
Hi Joseph:
For small areas the best Cutting Media in the market is
CCR1000/2000 from CCRCo, recyclable, @ 800.443.2726. Very low static
generator ( under 50V ). I would not use any cutting media for the whole
board. It would take way too long. It seems that your board coating is
too thick or the chemical stripper is too old.
Regards,
Ramon
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Joseph H. Smith
Sent: Wednesday, December 14, 2005 12:59 PM
To: [log in to unmask]
Subject: Re: [TN] senior chemist at HumiSeal
We use Humiseal 1A33 coating. Whe have used Humiseal 1063 stripper but
without much accomplished. Will take 8- 10 hours before anything
happens. This is just unacceptable. Other products have left residue
under BGA's or have been corrosive enough to pit solder joints or remove
component markings. Some semipastes or gel like products have left
residue under leads and so on and so on. So you see that is why I have
asked the question. Actually, bead blasting was a mechanically
technique that sound promising. Removed the coating quite fast but left
blasting media under some components that I could not wash out.
Andrew Kettlewell
-----Original Message-----
From: Edward Mines <[log in to unmask]>
To: [log in to unmask]
Sent: Wed, 14 Dec 2005 07:22:02 -0800 (PST)
Subject: senior chemist at HumiSeal
I was the senior chemist at HumiSeal for 12 years.
Different polyurethane conformal coatings require different strippers.
Do you know which one you was used? Is it yellow?
Be careful which stripper you use. Some of them can attack components.
Edward Mines BEChE, MEChE
238 Willard Dr.
Hewlett, NY 11557
516 205-6523
Yahoo! Shopping
Find Great Deals on Holiday Gifts at Yahoo! Shopping
___________________________________________________
Try the New Netscape Mail Today!
Virtually Spam-Free | More Storage | Import Your Contact List
http://mail.netscape.com
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
___________________________________________________
Try the New Netscape Mail Today!
Virtually Spam-Free | More Storage | Import Your Contact List
http://mail.netscape.com
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|