Dear Technetters
I look ovefr the IPC A-610 but I can not face with the quantity of nonwetting pads after assembly of the PCB.
What are the acceptibility criteria of nonwetting PCB for a PCB which
has about thousand pads both smd pads and through hole pads. Or, is there any standard which can state that after assembly
how many pads are tolerant to not being soldered per 1,000 pads.
Best Regards
--
Yusuf GÖMEÇ
Product Quality Engineer
BASKI DEVRE SAN ve TIC LTD STI
Ceyhan Sk. No:10 34896 Pendik-Istanbul-Turkey
Tel: 00 90 216 3901036 (4 Hat/Line)-173(Extention)
00 90 216 4836560 (4 Hat/Line)-173(Extention)
Fax: 00 90 216 3544941
00 90 216 4913269
Gsm: 00 90 533 6579897
00 90 533 7480014
--
Yusuf GÖMEÇ
Product Quality Engineer
BASKI DEVRE SAN ve TIC LTD STI
Ceyhan Sk. No:10 34896 Pendik-Istanbul-Turkey
Tel: 00 90 216 3901036 (4 Hat/Line)-173(Extention)
00 90 216 4836560 (4 Hat/Line)-173(Extention)
Fax: 00 90 216 3544941
00 90 216 4913269
Gsm: 00 90 533 6579897
00 90 533 7480014
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------