TECHNET Archives

December 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Mon, 5 Dec 2005 09:21:17 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Franklin Asbell <[log in to unmask]>
Subject:
From:
Franklin Asbell <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (105 lines)
Could it be residual mask from another lot due to poor equipment cleaning?
I've seen this a long time ago and we determined the coater was not
thoroughly cleaned allowing different type mask (usually the dried, caked on
gunk breaking loose and dropping into the new mask) to become mixed with
another making unusual patterns in the mask.

While the image is not exactly like what I recall, it is close. Since that
episode one learned to look into all the tight spaces during cleaning.

Franklin

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Stephen Gregory
Sent: Monday, December 05, 2005 8:49 AM
To: [log in to unmask]
Subject: Re: [TN] What is this solder mask defect?

Good Morning Everyone!

I got Wee Mei's picture up...go to:

http://stevezeva.homestead.com/files/Soldermask_Defect.JPG

I've seen this before, but I can't explain it either.

Kind Regards,

-Steve Gregory-

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Wee Mei
Sent: Sunday, December 04, 2005 6:58 PM
To: [log in to unmask]
Subject: [TN] What is this solder mask defect?

Steve,

Hello,

The suspect is completely flat and smooth to touch. An interesting
observation is that though it appear at the same location for all the
10pcs of board, the size of the image tend to get smaller and smaller if
the boards are arranged starting with the largest image. It can't be
soda strawing as it is not on trace. It can't be pink ring as it is not
around hole. What can it be? What is the likely cause?

Will ask Steve to put it up. Kindly take a look. Your opinion is greatly
appreciated.

Regards,
Wee Mei

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2