It is true that sprays have surfactant qualities, allowing the micelles
to adhere to neutral surfaces, through their lipophilic "end". The
hydrophilic end is therefore exposed to the air and, as they are
hygroscopic, they absorb moisture from the humidity in the air. It is
the monolayer of water molecules that is slightly conductive. Whether
such a coating would wash off or not depends on the strength of the
hydrogen bonding between the micelles and the substrate and whether
additional detergents are used in the wash process (sometimes
inadvertently as much tap/DI water contains ppms of surfactants).
Brian
Phil Nutting wrote:
> Has anybody used any of the available anti static sprays to reduce
> "static ticking" in a high voltage environment?
>
> On doing a web search I see there are many products on the market, but
> are these really for ESD control?. The question is, do I have to keep
> re-spraying the item to keep it functioning or is it a one time
> application?
>
> Thanks in advance.
>
> Phil Nutting
> Design for Manufacturing Engineer
> Kaiser Systems, Inc.
> 126 Sohier Road
> Beverly, MA 01915
> voice: 978-922-9300 x1310
> fax: 978-922-8374
> e-mail: [log in to unmask] <mailto:[log in to unmask]>
> www.kaisersystems.com <http://www.kaisersystems.com/>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>
--
______________________________________________
Please note new e-mail address [log in to unmask]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|