Hi suganthi
Dicy-cured FR-4 materials are traditionally composed of woven-glass
reinforcement materials and an epoxy resin with a
dicyandiamide (dicy) cure agent, dicy-cured FR-4
materials are commonly used in processes that use
Tin-Lead-based solder, such as automated-wave,
hot-air or hand-soldering assembly techniques.
Non-dicy resin technology in FR-4 or other resin laminates is
not new, even if dicy has been the preferred cross-linking
agent for many resin laminates. Non-dicy FR-4 laminates
have been aggressively investigated and marketed for several
years due largely to their improved thermal performance.
Thanks
On 12/28/05, Selva Suganthi <[log in to unmask]> wrote:
>
> Dear All,
>
> What is meant by DICY and NON - DICY Material?
>
> example DICY FR4
>
>
> Thanks and Regards
> Suganthi
>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16for additional information, or contact Keach Sasamori at
> [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
> "Progress is the activity of today and the assurance of tomorrow."
>
--
HARISH PS
98942 22433
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|