TECHNET Archives

December 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Fri, 23 Dec 2005 08:55:16 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Dave Dixon <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
Dave Dixon <[log in to unmask]>
Parts/Attachments:
text/plain (30 lines)
Good day all,
I want to wish each one of you a very Merry Christmas. If you don't 
celebrate the birth of Christ, I am really cool with that. I still wish
that 
the day that I call Christmas is a very merry one for you as well.
Dave

Engineers don't see the glass as half empty or half full. 
They see the glass as not designed properly. 
 
Dave Dixon
Engineering Technician
Aero-Mach Labs Inc.
7707 E. Funston Street
Wichita, KS     67207-3121
phone    316-682-7707
fax        316-219-2295
www.aeromach.com
 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2