TECHNET Archives

December 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Mon, 19 Dec 2005 11:58:51 -0500
Reply-To:
Subject:
From:
Tom Braswell <[log in to unmask]>
X-cc:
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (177 lines)
Mike,

You are correct!  And I use Indium 5.1 SAC for my SMT with excellent
results.  I have tested other Suppliers, but found that Indium has best
overall performance and appearance of my LF products.

Tom



-----Original Message-----
From: Mike Fenner [mailto:[log in to unmask]]
Sent: Friday, December 16, 2005 10:37 AM
To: [log in to unmask]
Subject: RE: [TN] Stencil Design for Lead-Free


A little note of caution: there is some "it depends" according to paste
supplier and possibly your board finish. It is true that with some a 1:1 is
required, due to lack of spread. Others you can use the same or pretty much
the same as your Sn/Pb. If you have a large stencil library this can be a
significant factor.


Regards

Mike Fenner
Indium Corporation

T: + 44 1908 580 400
M: + 44 7810 526 317
F: + 44 1908 580 411
E: [log in to unmask]
W: www.indium.com
Pb-free: www.Pb-Free.com



-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Tom Braswell
Sent: 16 December 2005 12:35
To: [log in to unmask]
Subject: Re: [TN] Stencil Design for Lead-Free

Joel,

I have been using 1:1 aps for our LF for some time with no problems.
We are printing 15mil & 20mil pitch with excellent solder wetting to pads
and leads.




Tom Braswell
Manufacturing Engineer
Fawn Electronics
6441 East NC 97
Elm City, NC 27822
Ph: (252) 977-8745
Fx: (252) 977-3477
Email: [log in to unmask]

************************************************************************
************************************************************************
**************************************************

This email is confidential and should only be viewed by the intended
recipient. If you received it in error, please reply to sender and delete
the message from your system.

All files contained are governed by Confidentiality between intended
parties, discussion of enclosed documents to outside parties other than
intended may be subject to legal actions.

************************************************************************
************************************************************************
**************************************************






-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Joel Mearig
Sent: Thursday, December 15, 2005 6:42 PM
To: [log in to unmask]
Subject: [TN] Stencil Design for Lead-Free


I am looking for information regarding stencil design for fine-pitch
lead-free applications. I am interested to see what most people are doing
for the aperture size. Are you reducing or going 1 to 1? If you are reducing
what is the reduction formula? Are you reducing the same regardless of
aperture stance to print direction? Any input would be much appreciated.



Joel Mearig

Delta Tau Data Systems, Inc.




---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per
day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------


***This email, its content and any files transmitted with it are intended
solely for the addressee(s) and may be legally privileged and/or
confidential. If you are not the intended recipient please delete and
contact the sender by return and delete the material from any computer. Any
review, retransmission, dissemination or other use of, or taking of any
action in reliance upon, this information by persons or entities other than
the intended recipient is prohibited.

Messages sent via this medium may be subject to delays, non-delivery and
unauthorized alteration. This email has been prepared using information
believed by the author to be reliable and accurate, but Indium Corporation
makes no warranty as to accuracy or completeness. In particular, Indium
Corporation does not accept responsibility for changes made to this email
after it was sent. Any opinions or recommendations expressed herein are
solely those of the author. They may be subject to change without notice.***



***This email, its content and any files transmitted with it are intended
solely for the addressee(s) and may be legally privileged and/or
confidential. If you are not the intended recipient please delete and
contact the sender by return and delete the material from any computer. Any
review, retransmission, dissemination or other use of, or taking of any
action in reliance upon, this information by persons or entities other than
the intended recipient is prohibited.

Messages sent via this medium may be subject to delays, non-delivery and
unauthorized alteration. This email has been prepared using information
believed by the author to be reliable and accurate, but Indium Corporation
makes no warranty as to accuracy or completeness. In particular, Indium
Corporation does not accept responsibility for changes made to this email
after it was sent. Any opinions or recommendations expressed herein are
solely those of the author. They may be subject to change without notice.***

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2