hi,
the problem here, with hard anodizing, is that these connector shells
need to be electrically grounded.
phil
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Brian Ellis
Sent: Thursday, December 15, 2005 4:35 AM
To: [log in to unmask]
Subject: Re: [TN] Really Terrible Looking Chem Film...
I concur. However, if you want something that looks cosmetically better,
you should ask your supplier to hard-anodise and seal the parts in
boiling water for 30 minutes. This will resist alkaline cleaners (pH
<12) much better than conversion coatings (and can be dyed in a very
wide range of beautiful colours, to boot!).
Brian
Stephen Gregory wrote:
> Hi All!
>
> We have a series of boards that we build here, that we've been
> building for years and years.
>
> These boards use a 320-pin right-angle male connector that has an
> aluminum chem-filmed body.
>
> After building the last batch of boards, we have 5-assemblies that
> have the worst looking chem-film coating on the connectors I have ever
seen. Check out:
>
> http://stevezeva.homestead.com/files/Chem_Film_Gone_Bad.jpg
>
> I'm not a chem-film guru by any means, but I have a hard time
> believing that anything in my process caused this appearance.
> Chem-film conversion coatings are permanent aren't they? I mean the
> only way to remove them is mechanically, or etch them, right?
>
> These boards were wave soldered with a RMA flux and cleaned in Kyzen
> Aquanox 4512P.
>
> Anybody seen this before and know what might cause this?
>
>
> Stephen Gregory
> Senior Process Engineer
> LaBarge Incorporated
> Tulsa, OK 74146
> (918) 459-2285
> (918) 459-2350 FAX
> _______________________________________________________
> This message may contain information that is privileged and
confidential to LaBarge, Inc. It is for use only by the individual or
entity named above. If you are not the intended recipient, you may not
copy, use or deliver this message to anyone. In such event, you should
destroy the message and kindly notify the sender by reply e-mail.
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
> unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
> or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
> archives of previous posts at: http://listserv.ipc.org/archives Please
> visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at
> [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>
--
______________________________________________
Please note new e-mail address [log in to unmask]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|