The same can be said of most stripping agents. Thorough cleaning of
stripped assemblies is vital.
Doug Pauls
- Bogert
<[log in to unmask]>
Sent by: TechNet To
<[log in to unmask]> [log in to unmask]
cc
12/14/2005 04:07 Subject
AM Re: [TN] Help with removing UR
Conformal Coating
Please respond to
TechNet E-Mail
Forum
<[log in to unmask]>
; Please respond
to
- Bogert
<[log in to unmask]>
Never use Humiseal Type conformal coating remover. This stuff is
conductive and can become trapped under components causing problems.
----- Original Message -----
From: Dehoyos, Ramon<mailto:[log in to unmask]>
To: [log in to unmask]<mailto:[log in to unmask]>
Sent: Tuesday, December 13, 2005 10:35 AM
Subject: Re: [TN] Help with removing UR Conformal Coating
Hi Andrew:
Humiseal makes a UR stripper but it will remove
all the coating vertically in significantly quicker time than horizontally.
Under the BGAs it will remove it if the coating did not fill all the
spacing under the BGA. If there is a complete fill of the spacing under the
BGA, it is a different story because the horizontal distance is much
greater. Perhaps damming the BGA and filling with the chemical may
accomplish what you want. I would try it on a scrap board that is made of
the same material. Cheers
Regards,
Ramón
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Joseph H. Smith
Sent: Tuesday, December 13, 2005 9:48 AM
To: [log in to unmask]<mailto:[log in to unmask]>
Subject: [TN] Help with removing UR Conformal Coating
Has anyone had experience or success with removing conformal coating for
PWA that has been coated with UR coating especially using a chemical means.
I am particularly interested with how you handled coating around or under
BGA's.
Any help would be grateful.
Thanks.
Andrew Kettlewell
Process Engineer
Sypris Electronics
Tampa, FL
___________________________________________________
Try the New Netscape Mail Today!
Virtually Spam-Free | More Storage | Import Your Contact List
http://mail.netscape.com<http://mail.netscape.com/>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask]<mailto:[log in to unmask]>
with following text in the BODY (NOT the subject field): SIGNOFF Technet To
temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]<mailto:[log in to unmask]>: SET Technet NOMAIL or (MAIL) To
receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]<mailto:[log in to unmask]>: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives<
http://listserv.ipc.org/archives> Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16<
http://www.ipc.org/contentpage.asp?Pageid=4.3.16> for additional
information, or contact Keach Sasamori at [log in to unmask]<
mailto:[log in to unmask]> or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask]<
mailto:[log in to unmask]> with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]<mailto:[log in to unmask]>: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]<mailto:[log in to unmask]>: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives<http://listserv.ipc.org/archives>
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16<
http://www.ipc.org/contentpage.asp?Pageid=4.3.16> for additional
information, or contact Keach Sasamori at [log in to unmask]<
mailto:[log in to unmask]> or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|