John,
Let me add to what Jeffrey has said by pointing out that the plated thickness uniformity must be reasonably close so that the values you are assigning will have validity. I've seen plated thickness uniformity vary from 1.1 mils to over 3.0 mils on the same board. I hope others will weigh in on this because I'm told plated thickness can significantly affect the impedance values.
Roger Mouton
EIMC - Advanced Plating Technologies
949 481-5194
www.smartcatshield.com
[log in to unmask]
-------------- Original message from Babcock John <[log in to unmask]>: --------------
> Hi All,
>
> When figuring impedances with the field solvers...for the external layer
> copper thickness does one enter the finished plated value or the
> unfinished?
>
> If you specify a top and bottom layer as 1.5 oz plated to 2 oz, which
> value would you put into the field solver for the impedance calc?
>
> I would figure you put in the finished plated value...but not positive.
>
> Thanks!
>
> John
> PCB Designer III
> Isothermal Systems Research
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
> additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
> -----------------------------------------------------
|
|
|