Ron,
I don't know if this will help you but if the PCB vendor is UL certified the
laminate will have both a max operating temperature, usually between 100-130
deg C for FR-4 and also carry a UL-94 flame rating
(http://www.ul.com/plastics/flame.html) typically 94V-0.
John Parsons
-----Original Message-----
From: DesignerCouncil [mailto:[log in to unmask]] On Behalf Of Scott,
Ron
Sent: Thursday, December 08, 2005 3:07 PM
To: [log in to unmask]
Subject: [DC] Flammability of FR4
All,
I have a customer that is having an isuue with their boards bursting
into flame when using one of our devices. Our device comes in two
flavors, TQFP & QFN. The QFN is the device that ignites the board. My
question is: Does FR4 have a flash point? I'm quite familiar with Tg
ratings but I haven't heard about a flash point. Is there such a thing?
If so, where can I find information? Manufacturer will not reveal board
material to me.
Cheers,
Ron Scott C.I.D.
Texas Instruments
Storage Products Group
Tel: 214.567.4715
Cell: 972.816.7978
Fax: 972.761.5070
[log in to unmask]
---------------------------------------------------------------------------------
DesignerCouncil Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
To temporarily stop/(restart) delivery of DesignerCouncil send: SET DesignerCouncil NOMAIL/(MAIL)
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
---------------------------------------------------------------------------------
|
|
|