Subject: | |
From: | |
Reply To: | |
Date: | Tue, 15 Nov 2005 20:21:20 -0600 |
Content-Type: | text/plain |
Parts/Attachments: |
|
|
Either ENIG or immersion silver will give you a very flat finish.
Ken Kirby
Applications Engineer
Speedline Technologies
573-317-3062
cell 817-946-3357
Babcock John
<JBabcock@SPRAYCO
OL.COM> To
Sent by: TechNet [log in to unmask]
<[log in to unmask]> cc
Subject
11/15/05 06:28 PM [TN] best plated surface finish
Please respond to
TechNet E-Mail
Forum
<[log in to unmask]>
; Please respond
to
Babcock John
<JBabcock@SPRAYCO
OL.COM>
If somebody wants an extra smooth plating finish using lead free plating
what material would they use...and what would be the finishing process?
I've heard HASL is sort of rough...and it really doesn't apply using
silver solder because of the melting temps.
Is ENIG (electroless nickel immersion gold) the way to go to get a
smooth finish?
thanks!
John Babcock
PCB Designer III
Isothermal Systems Research (ISR)
2218 N. Molter Rd
Liberty Lake, WA 99019
[log in to unmask]
P: (509) 241-4641
F: (509) 444-1082
This E-mail and any files transmitted with it are confidential and
proprietary in nature and intended solely for the use of the individual
to whom it is addressed. If you have received this E-mail in error,
please send it back to the person that sent it to you. Any views or
opinions presented are solely those of its author and do not necessarily
represent those of Isothermal Systems Research, Inc. Unauthorized
publication, use, dissemination, forwarding, printing or copying of this
email and its associated attachments is strictly prohibited. Thank you
for your cooperation.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|