Hi Vladimir,
Which part of
"All fatigue models, not just for solder, are empirical models. Because no
such model can take into account all possible variables, they concentrate on
1st-order parameters, and some 'adjustments' for 2nd-order influences.
The Coffin-Manson model is empirical, and even a simplification of the more
comprehensive, but still empirical, Morrow model--both of these only take into
account fatigue from plastic deformation (low-cycle fatigue). The Basquin
equation is empirical--taking into account only fatigue from elastic deformation
(high-cycle fatigue). In the early days of fatigue studies [and early days
lasted into the 60's], nobody even dreamed of using material in cyclic loading
that was high enough to cause plastic deformation (yielding). Both of these
models are only for non-creeping metals. The Engelmaier-Wild model, and others for
solder, take the plastic deformation resulting from creep into consideration.
If you combine the Coffin-Manson and Basquin equations, you wind up with
something like the Engelmaier model on which ASTM E 796 “Standard Test Method for
Ductility Testing of Metallic Foil” and the modeling for both flexible
circuitry and plated-through vias are based.
I am certainly aware that 'scientists' have been bothered by the fact that
fatigue models cannot be developed from first principles--but I rather have
empirical models than a repeat of the 'Comet' jet liner disasters. The difference
between 'scientists' and 'engineers' is that the latter have to make decisions
and build product based on incomplete information."
do you disagree with?
We have been successfully been building product using these models since the
'60's.
Regards,
Werner Engelmaier
Engelmaier Associates, L.C.
Electronic Packaging, Interconnection and Reliability Consulting
7 Jasmine Run
Ormond Beach, FL 32174 USA
Phone: 386-437-8747, Fax: 386-437-8737, Cell: 386-316-5904
E-mail: [log in to unmask], Website: www.engelmaier.com
-------------------------------------------------------------------------------Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-------------------------------------------------------------------------------
|