Seal the PCA if you have any questions about moisture driven performance
issues..
In the best case...Moisture will make the lossy sheet resistors out of
your PCB surface...
In the worst case...You will grow junk...
Paul
Paul Edwards
Process Engineering
[log in to unmask]
Tel: 408-433-4700
FAX: 408-433-9988
Surface Art Engineering
81Bonaventura Dr.
San Jose, CA 95134
DUNS: 944740570
CAGE/NCAGE: 1XZ48
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Eric CHRISTISON
Sent: Tuesday, November 29, 2005 9:34 AM
To: [log in to unmask]
Subject: Re: [TN] Humidity and enclosed RF board
Agree with Richard about the environment. Letting the enclosure breathe
is
also a good plan; how many mobile phones fail due to humidity related
failures?
You might also consider adding a breathing desiccator to the enclosure
although they tend to be expensive and need replaced every six moths or
so.
Regards,
Eric Christison
Mechanical Engineer
Home, Personal, Communication Sector - Imaging Division
STMicroelectronics
33 Pinkhill
Edinburgh
EH12 7BF
Tel: +44 (0)131 336 6165
Fax: +44 (0)131 336 6001
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard
> Sent: Tuesday, November 29, 2005 5:25 PM
> To: [log in to unmask]
> Subject: Re: [TN] Humidity and enclosed RF board
>
>
> It also depends on the environment where the box will live.
> If it is near the sea, there is a much higher probability of
> failure if any moisture does enter from outside.
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Douglas O. Pauls
> Sent: Tuesday, November 29, 2005 11:01 AM
> To: [log in to unmask]
> Subject: Re: [TN] Humidity and enclosed RF board
>
> Well, it depends.
>
> You say that the casing seals the electronics from the
> external atmosphere. How well? Is it a hermetic seal? Are
> you using an elastomeric gasket? Do you package with an inert
> cover gas? What is the design life of the product and what
> are the consequences of failure?
>
> In my experience, even those enclosures assumed to be
> "hermetic" are not, and that usually means moisture will
> eventually get in and will have a hard time getting back out.
> So it all depends on how well insulated your case keeps the
> electronics throughout the design life. Elastomeric gaskets
> willl wear out. Field repair is often less than optimal.
>
> If moisture gets inside the case, it will condense on your
> boards when you go through dew point. Can it grow dendrites?
> Yes. What is the risk? It Depends. Dendrites have been
> observed to grow in as little as 3.5 volts DC. There is no
> "safe" level of humidity because the degree of risk is
> dependent on both humidity and the amount of ionic soil. The
> dirtier it is, the less humidity it takes. Some papers have
> suggested 70% RH as a threshold, but this is usually SIR type
> of testing, not field trials. In addition, if your product
> is functioning in some of the more polluted areas of the
> world, and the enclosure is not hermetic, then the pollutant
> gasses also get into the enclosure and do nasty things.
>
> Doug Pauls
>
>
>
>
> "Tempea, Ioan"
> <itempea@POSITRON
> .QC.CA>
> To
> Sent by: TechNet [log in to unmask]
> <[log in to unmask]>
> cc
>
>
> Subject
> 11/29/2005 10:43 [TN] Humidity and enclosed RF
> board
> AM
>
>
> Please respond to
> TechNet E-Mail
> Forum
> <[log in to unmask]>
> ; Please respond
> to
> "Tempea, Ioan"
> <itempea@POSITRON
> .QC.CA>
>
>
>
>
>
>
> Hi Technos,
>
> application: one RF board and one antenna, no conformal
> coating, both sealed inside of a casing; outdoor unit, will
> see temp and humidity variations.
>
> question: assuming that the boards are well insulated from
> the exterior, should I worry about long term rel of the
> boards? Otherwise said, due to temp variations, can the
> residual humidity inside the casing condensate on the boards
> and cause damage? Or can it make grow dendrites?
>
> And a general question: For dendrites we need a potential
> difference, humidity and dirt; is there any threshold for the
> humidity level, below which dendrites will not grow?
>
> Thank you,
> Ioan
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV
> 1.8e To unsubscribe, send a message to [log in to unmask] with
> following text in the BODY (NOT the subject field): SIGNOFF
> Technet To temporarily halt or
> (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE
> mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit
IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|