My apologies for being about to point out what perhaps to you is obvious,
but it's not clear if you are going from
- RMA with no cleaning
- RMA with solvent cleaning
- RMA with semiaqeous cleaning
IF you are already semi-aqueous cleaning it's a small step to 100% water
wash and you end up with a simplified process.
IF you are not presently cleaning this is a big step you are proposing. Even
from solvent cleaning it's a significant change as water is very different
in its behaviour from solvent. [Basically it doesn't want to be dry and its
higher surface tension makes for different behaviour.] In this case the
last thing to worry about is process validation/control.
You have to make sure that your assemblies can be water washed: components
are sealed, no water traps caused by geometries of board and components, no
sleeved wires, gaps under devices can be flushed though and so on. Can
assemblies stand drying cycle and so on. Even things like labels not being
water proof can catch you out.
Regards
Mike Fenner
Indium Corporation
T: + 44 1908 580 400
M: + 44 7810 526 317
F: + 44 1908 580 411
E: [log in to unmask]
W: www.indium.com
Pb-free: www.Pb-Free.com
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Brian Ellis
Sent: 22 November 2005 14:35
To: [log in to unmask]
Subject: Re: [TN] Water Soluble Flux
You qualify it initially by SIR/ECMR testing, possibly IC analysis. Once you
have qualified the product and the process, you can then test a number of
identical assemblies in an ionic contamination tester to establish a process
control baseline (mean and standard deviation) for that type of assembly. If
subsequent production testing falls into the same mean and standard
deviation envelope, you can go to bed at night and sleep soundly on both
ears. I recommend this qualification be repeated, say, annually, to cater
for variations.
Brian
Long, Thomas - Avionics wrote:
> I am looking for some advice on qualifying a process for
> switching from RMA flux to water soluble flux. I am aware that a
> large company learned through SIR testing (too late) that when
> switching from RMA to water soluble their cleaning process was not
> effectively cleaning all of the flux residues off and it was causing
> performance issues. The company actually had to scrap product and
> revisit type of flux and cleaning. I'm not sure if organic flux
> residues can be detected with omegameter cleanliness testing and this
product is class 3 high rel.
>
> I appreciate any input and experiences that anyone can share.
>
> Tom Long
> ITT Avionics
***This email, its content and any files transmitted with it are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient please delete and contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination or other use of, or taking of any action in reliance upon, this information by persons or entities other than the intended recipient is prohibited.
Messages sent via this medium may be subject to delays, non-delivery and unauthorized alteration. This email has been prepared using information believed by the author to be reliable and accurate, but Indium Corporation makes no warranty as to accuracy or completeness. In particular, Indium Corporation does not accept responsibility for changes made to this email after it was sent. Any opinions or recommendations expressed herein are solely those of the author. They may be subject to change without notice.***
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|