I am looking for some advice on qualifying a process for
switching from RMA flux to water soluble flux. I am aware that a large
company learned through SIR testing (too late) that when switching from
RMA to water soluble their cleaning process was not effectively cleaning
all of the flux residues off and it was causing performance issues. The
company actually had to scrap product and revisit type of flux and
cleaning. I'm not sure if organic flux residues can be detected with
omegameter cleanliness testing and this product is class 3 high rel.
I appreciate any input and experiences that anyone can share.
Tom Long
ITT Avionics
************************************
This e-mail and any files transmitted with it are proprietary and intended solely for the use of the individual or entity to whom they are addressed. If you have received this e-mail in error please notify the sender. Please note that any views or opinions presented in this e-mail are solely those of the author and do not necessarily represent those of ITT Industries, Inc. The recipient should check this e-mail and any attachments for the presence of viruses. ITT Industries accepts no liability for any damage caused by any virus transmitted by this e-mail.
************************************
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|