Bob,
As a supplier, I recommend you contact them if you have concerns.
But fyi,Sn-Bi is our std terminal plating for smaller parts.We have no
reliability issues with Bi.Some customers require it because they
believe it helps to prevent Tin Whiskers.
And according to an IPC sponsored seminar I attended,the concentrations
required to produce low temp melting ophase ar nowhere near as small as
the concentations produced by the 3% Bi contained in a typical Sn-Bi
terminal plating.
Regards
Dennis Becker
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bob Barr
Sent: Tuesday, November 01, 2005 3:33 PM
To: [log in to unmask]
Subject: [TN] SnBi Lead Plating
We received a last time buy notice from a distributor for a NEC part.
The part is going to a RoHS compliant finish. The information we
received seems to indicate the lead finish will be SnBi. With the
transition from Pb to Pb-free still happening, it seems like a problem
to have Bi on a component lead. Everything I have read says Bi cannot be
mixed with Pb because it forms a low temperature melting alloy. Has
anybody heard of Bi being used in a component lead finish? I'm hoping
this may just be a mis- communication.
Thanks.
Bob
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
This message is processed by the PrivaWall Email Security Server.
The information contained in this communication is proprietary to Israel Aircraft Industries Ltd.
and/or third parties, may contain confidential or privileged information, and is intended only for
the use of the intended addressee thereof. If you are not the intended addressee, please be aware
that any use, disclosure, distribution and/or copying of this communication is strictly prohibited.
If you receive this communication in error, please notify the sender immediately and delete it from
your computer. Thank you.
This message is processed by the PrivaWall Email Security Server.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|