TECHNET Archives

November 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Steve Hodge <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Steve Hodge <[log in to unmask]>
Date:
Tue, 15 Nov 2005 07:38:33 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (44 lines)
Jim, send me the stack-up specifics and I will check the model for you. I
have 2 different modeling programs.


At 07:28 AM 11/15/2005, you wrote:
>Hello,
>
>If there are any impedance testing gurus out there I have a question for
>you.  We are testing an edge coupled offset strip line coupon.  We modeled
>the stack up to give us 100 ohms differential.  When we test the coupon we
>get around 130 ohms.  We have done a microsection of the coupon and modeled
>the coupon data and Polar says we should have 105 ohms, within tolerance.
>We had a 4 panel lot and it is consistent across the board.  The coupon is
>constructed correctly.  My question is, other than what I am seeing on the
>microsection should I look for to find the culprit of the high reading?  Any
>help would be great.
>
>Jim Henderson
>Colonial Circuits
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>for additional information, or contact Keach Sasamori at [log in to unmask] or
>847-615-7100 ext.2815
>-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2