Carl,
To answer both of your questions, SEM/EDS analysis is a good way to see if
it's a Pb-free solder or Sn/Pb solder. If you have XRF with elemental
characterization capability, that should work as well. The instrument
chambers should accomodate most sizes. If not, a tiny amount of solder can
be removed from one location for SEM/EDS analysis.
Hans Shin
Pacific Testing Laboratories, Inc.
www.pacifictesting.com
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Carl VanWormer
Sent: Tuesday, November 01, 2005 8:27 AM
To: [log in to unmask]
Subject: [TN] Lead-Free testing
Is there an easy way to verify that an assembly has been produced with
lead-free solder? Conversely, is there a quick and easy test for lead in a
solder joint?
Carl Van Wormer
Cipher Systems
1800 NW 169th Place, Suite B-100
Beaverton, OR 97006
Phone (503)-617-7447 Fax (503)-617-6550
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|