Hi Steve, it was nice talking to you at the WORKS conference. As you probably are aware, the PWA's you make for DRS-M have a higher level document (MIL-C-23200) invoked than J-STD-00 or IPC-A-610. The MIL-C-23200 document mandates that if a part specification mandates that part marking be permanent, then no subsequent processing (e.g., cleaning, soldering, etc.) can cause the markings to be obliterated.
The problem you are having is not unique. We have other folks who are having the same problem.
The only option I am aware of is for you to determine if the specification for the part requires the marking to be permanent. If so, then obtain corrective action from the part manufacturer. Other option would be to add a label or otherwise mark with the missing information. Other option would be to disposition as a nonconforming condition for DRS resolution.
I have had several discussions/arguments with the IPC regarding marking requirements in 001 and 610. I maintained that important markings such as the P/N, polarity markings, reference designation markings and markings that designate the part has been electrical screen tested should not be obliterated by any processing method. I have always lost the argument. That is why we mandate no loss of these type markings.
----- Original Message -----
From: Steve Gregory<mailto:[log in to unmask]>
To: [log in to unmask]<mailto:[log in to unmask]>
Sent: Friday, November 04, 2005 10:04 AM
Subject: [TN] Component marking on metal parts...
Happy Friday All!
We've got a rather irritating problem here that is starting to become more
than just
irritating, it's become a real issue. It has to do with part marking.
J-STD-001 states:
9.2 Marking Assembly identification such as part numbers and serial numbers
shall
remain legible (capable of being read and understood) after all tests,
cleaning and
other processes to which the item is subjected.
Additional markings (such as labels added during the manufacturing process)
should
not obscure the original supplier's markings.
Individual component markings, reference designators and polarity
indicators should
remain legible and components should be mounted in such a manner that
markings
are visible.
The only parts that we have a problem with are metal parts such as hybrids
or DC\DC
converters. We clean with Kyzen and have a real problem with the markings
coming off
in wash. We try to protect them with a piece of kapton tape, but that only
works hit and miss.
Does anybody else have the same problem? What have you done to protect the
part
markings?
Kind regards,
-Steve Gregory-
Senior Process Engineer
LaBarge Incorporated
Tulsa, Oklahoma
(918) 459-2285
(918) 459-2350 FAX
__________________________________________________________________
This message may contain information that is privileged and confidential to
LaBarge, Inc. It is for use only by the individual or entity named above.
If you are not the intended recipient, you may not copy, use or deliver
this message to anyone. In such event, you should destroy the message and
kindly notify the sender by reply e-mail.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask]<mailto:[log in to unmask]> with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]<mailto:[log in to unmask]>: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]<mailto:[log in to unmask]>: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives<http://listserv.ipc.org/archives>
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16<http://www.ipc.org/contentpage.asp?Pageid=4.3.16> for additional information, or contact Keach Sasamori at [log in to unmask]<mailto:[log in to unmask]> or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|