TECHNET Archives

November 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Fri, 4 Nov 2005 11:35:17 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Content-type:
text/plain; charset=us-ascii
Subject:
From:
Steve Gregory <[log in to unmask]>
X-cc:
MIME-Version:
1.0
Parts/Attachments:
text/plain (196 lines)
Hi Kat!

It's not labels that we have the problem with, but the ink-stamped or
painted markings on metal parts...and we've always been fighting
this problem to a certain degree.

It's just that now it seems we're building a lot of assemblies for a
customer
that use these types of parts, and they're real picky when it comes to
markings,
only because their customer is.

We use Kyzen Aquanox 4512P in a Aqueous Technologies SMT800 batch cleaner.
We run the concentration from 10-20%, at a wash temp of 140 F. The rinse is
ambient
temp DI water.

Almost every one of these assemblies get conformal coated with urethane
coating.
So we try and make sure the boards are as pristine as possible prior to
coating.

Kind regards,

-Steve Gregory-
Senior Process Engineer
LaBarge Incorporated
Tulsa, Oklahoma
(918) 459-2285
(918) 459-2350 FAX



|---------+---------------------------->
|         |           Kathy Kuhlow     |
|         |           <[log in to unmask]
|         |           M>               |
|         |           Sent by: TechNet |
|         |           <[log in to unmask]>|
|         |                            |
|         |                            |
|         |           11/04/2005 10:46 |
|         |           AM               |
|         |           Please respond to|
|         |           TechNet E-Mail   |
|         |           Forum            |
|         |           <[log in to unmask]>|
|         |           ; Please respond |
|         |           to Kathy Kuhlow  |
|         |           <[log in to unmask]
|         |           M>               |
|         |                            |
|---------+---------------------------->
  >--------------------------------------------------------------------------------------------------------------|
  |                                                                                                              |
  |       To:       [log in to unmask]@SMTP@Exchange                                                                |
  |       cc:       (bcc: Stephen R Gregory/LABARGE)                                                             |
  |       Subject:  Re: [TN] Component marking on metal parts...                                                 |
  >--------------------------------------------------------------------------------------------------------------|



Is the label a just poly or is it  kapton backed? The ink probably is not
thermally burnt in but printed on it. What kyzen are you using? I had found
that the Ionox 3330 does  a really good job with maintaining poly labels
with printed ink on transformers and relays (spray over immersion). What
wash process are you using (in-line spray over spray, spray over immersion,
or batch table top)?  What concentration?  Is this a new problem on a
specific lot number or has this always been something that you have always
dealt with?

Kat

>>> [log in to unmask] 11/4/2005 10:33:45 AM >>>


        Hi Steve:
        It has to do with the part manufacturer not properly cleaning
the parts  prior to marking them. Some one is cutting corners. That is
the root cause of the problem. It is a pain to ensure the manufacturer
does a better job in marking the parts, but it would be a permanent
solution without introducing more process steps in your facility for
other people's laziness, or make them place labels such as Brady labels.
They stay on very well, even on dirty metal.
        Regards,
        Ramon

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Friday, November 04, 2005 10:05 AM
To: [log in to unmask]
Subject: [TN] Component marking on metal parts...

Happy Friday All!

We've got a rather irritating problem here that is starting to become
more than just irritating, it's become a real issue. It has to do with
part marking.

J-STD-001 states:

9.2 Marking Assembly identification such as part numbers and serial
numbers shall remain legible (capable of being read and understood)
after all tests, cleaning and other processes to which the item is
subjected.

Additional markings (such as labels added during the manufacturing
process) should not obscure the original supplier's markings.

Individual component markings, reference designators and polarity
indicators should remain legible and components should be mounted in
such a manner that markings are visible.

The only parts that we have a problem with are metal parts such as
hybrids or DC\DC converters. We clean with Kyzen and have a real problem
with the markings coming off in wash. We try to protect them with a
piece of kapton tape, but that only works hit and miss.
Does anybody else have the same problem? What have you done to protect
the part markings?

Kind regards,

-Steve Gregory-
Senior Process Engineer
LaBarge Incorporated
Tulsa, Oklahoma
(918) 459-2285
(918) 459-2350 FAX
__________________________________________________________________
This message may contain information that is privileged and confidential
to LaBarge, Inc.  It is for use only by the individual or entity named
above.
If you are not the intended recipient, you may not copy, use or deliver
this message to anyone.  In such event, you should destroy the message
and kindly notify the sender by reply e-mail.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------



__________________________________________________________________
This message may contain information that is privileged and confidential to
LaBarge, Inc.  It is for use only by the individual or entity named above.
If you are not the intended recipient, you may not copy, use or deliver
this message to anyone.  In such event, you should destroy the message and
kindly notify the sender by reply e-mail.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2