TECHNET Archives

November 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Wed, 30 Nov 2005 15:32:00 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Sherif Refaat <[log in to unmask]>
Subject:
From:
Sherif Refaat <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Comments:
RFC822 error: <W> MESSAGE-ID field duplicated. Last occurrence was retained.
Parts/Attachments:
text/plain (122 lines)
One way to stop the solder wicking without plugging or tenting the via holes is to extend the solder mask, so it would cover the via pad without encroaching on the via hole itself. This way there will be a wider dam of solder mask that should be enough to prevent the solder thieving.


Sherif Refaat, Eng.

Technology Roadmap Consultants Inc.

E-mail: [log in to unmask]

Tel. (514) 624 9842

Fax (514) 624 0091



> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard
> Sent: Wednesday, November 30, 2005 3:59 PM
> To: [log in to unmask]
> Subject: Re: [TN] Plugging vias necessary?
> 
> Without the plug, the solder from the sphere can wet down into the
> adjacent via to the backside of the pwb during reflow.
> On a dogbone pattern, with one side the pad and the other side the
> connecting via, the small soldermask dam that goes over the thinnest
> part of the dogbone pattern is not enough to stop the solder wicking.
> The solder will wick right under that flimsy little dam, and the via
> will rob the solder. This is called solder thieving. The soldermask plug
> prevents that from happening. If you ever need to rework that BGA, the
> site prep operation nearly always makes the little soldermask dam worse,
> and after you replace the part you get even more solder thieving, and
> the entire rework/X-ray/test/rework cycle spins on down into a black
> hole called scrap. One almost never sees BGAs with daisychained dogbones
> without the soldermask plug, and that is a good thing, as Martha says.
> 
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Black, Paul
> Sent: Wednesday, November 30, 2005 7:50 AM
> To: [log in to unmask]
> Subject: [TN] Plugging vias necessary?
> 
> Hi Everyone,
> 
> I have a board with a 357 pin PBGA. Each pad has a short etch leading to
> an adjacent via. Currently, the fabrication drawing calls for each via
> to be plugged. The assembly process for this board does not contain a
> wave solder step and the test engineer assures me that plugging the vias
> is not necessary for vacuum during incircuit testing, so is there some
> other reason for plugging these vias? They are plugged with soldermask,
> and I feel like we are unnecessarily introducing potential problems into
> the process.
> 
> Thanks in advance for your opinions.
> 
> Paul Black
> Manufacturing Engineer
> Kronos
> [log in to unmask]
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
> unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
> (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
> archives of previous posts at: http://listserv.ipc.org/archives Please
> visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
> additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
> unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
> (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
> archives of previous posts at: http://listserv.ipc.org/archives Please
> visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
> additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
> 
> 
> This message is processed by the PrivaWall Email Security Server.
> 
> 
> 
> 
> 
> The information contained in this communication is proprietary to Israel Aircraft Industries Ltd.
> and/or third parties, may contain confidential or privileged information, and is intended only for
> the use of the intended addressee thereof. If you are not the intended addressee, please be aware
> that any use, disclosure, distribution and/or copying of this communication is strictly prohibited.
> If you receive this communication in error, please notify the sender immediately and delete it from
> your computer. Thank you.
> 
> 
> This message is processed by the PrivaWall Email Security Server.
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
> -----------------------------------------------------

ATOM RSS1 RSS2