TECHNET Archives

November 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Ingemar Hernefjord <[log in to unmask]>
Date:
Wed, 30 Nov 2005 09:20:58 -0000
Reply-To:
Subject:
From:
Mike Fenner <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
<000001c5f4df$ccfec460$a97b65d5@MONKEY>
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (172 lines)
From information given the IDQ (It Depends Quotient)  in any answer would be
too high. To give a useful answer need more information to bring the IDQ
down. :)

Need to know actual plated thicknesses of Au Ag etc, also what and how much
of what is plated  under the Au Ag etc on what basis metal. 




Regards

Mike Fenner
Indium Corporation

T: + 44 1908 580 400
M: + 44 7810 526 317
F: + 44 1908 580 411
E: [log in to unmask]
W: www.indium.com
Pb-free: www.Pb-Free.com



-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ingemar Hernefjord
Sent: 29 November 2005 12:24
To: [log in to unmask]
Subject: [TN] SV: [TN] SV: [TN] Soldering gold and silver together

So, the silver 'ring' does not participate in the physical action, just
works like a distance. If you degold the pins before soldering, I can't see
any problems. Must say you have a uniqe project!

Additional: depending on what current and contact resistance you talk about,
I would prefer brazing the parts together, but it may not be possible with
your application ? Mike Fenner will probably have a word here..

Ingemar

-----Ursprungligt meddelande-----
Från: TechNet [mailto:[log in to unmask]] För TUGMEN UNSAL (MIKES INTERNET)
Skickat: den 29 november 2005 12:58
Till: [log in to unmask]
Ämne: Re: [TN] SV: [TN] Soldering gold and silver together

WE HAVE CONTACT LANDS (GOLD PLATED BRASS) SOLDERED ON A PCB. AND THEY HAVE A
MATE WITH RECIPROCAL SPRING CONTACTS AS A POWER SWITCH.

WE NEED TO ELEVATE THE CONTACT LANDS TO DECREASE THE CONTACT RESISTANCE.
SO WE USED A RING (SILVER PLATED) BETWEEN THE PCB AND CONTACT LAND (GOLD
PLATED) BEFORE SOLDERING THEM. DOES THIS SITUATION CAUSE ANY PROBLEM ?

I THINK WE CAN'T USE ANY PLASTIC RING BECAUSE OF THE SPRING PRESSURE (FROM
THE OPPOSITE PART) AND THE SOLDERING CONSTRAINTS.

THANK YOU FOR YOUR HELP INGEMAR..

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ingemar Hernefjord
Sent: Tuesday, November 29, 2005 12:30 PM
To: [log in to unmask]
Subject: [TN] SV: [TN] Soldering gold and silver together

Jewellers have joined gold and silver together back to keltic practice, so
it works nice as a gem, but you have to do with connectors, i.e.
current and voltage and maybe even humidity and heat. Using tin, you will
get some intermetallics and maybe brittle joints. When you
connect/disconnect the parts there may be some uncalculated forces.
Manipulating connectors is a dubious thing, depending on what pins you are
talking about: subminiature? Signal? Power? I think most of us would like to
see a photo and some more technical information. Ask Steve to put a pic on
the wall before you go on.

Why do you need a metallic ring? Can't you use some 'plastic' distance
rings? 
Inge

-----Ursprungligt meddelande-----
Från: TechNet [mailto:[log in to unmask]] För TUGMEN UNSAL (MIKES INTERNET)
Skickat: den 29 november 2005 10:52
Till: [log in to unmask]
Ämne: [TN] Soldering gold and silver together

Dear all,

We put silver plated ring on the connectors pin to be able to lift up
connectors from PCB. Connector pins are gold plated.
Is it possible to solder (tin) a gold plated and a silver plated material
together ? Two of them can be soldered individually, but can they be
soldered together using tin ?
Any problems we may face to kd

Thank you.  
Tugmen.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per
day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information,
or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per
day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information,
or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per
day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information,
or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------


***This email, its content and any files transmitted with it are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient please delete and contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination or other use of, or taking of any action in reliance upon, this information by persons or entities other than the intended recipient is prohibited. 

Messages sent via this medium may be subject to delays, non-delivery and unauthorized alteration. This email has been prepared using information believed by the author to be reliable and accurate, but Indium Corporation makes no warranty as to accuracy or completeness. In particular, Indium Corporation does not accept responsibility for changes made to this email after it was sent. Any opinions or recommendations expressed herein are solely those of the author. They may be subject to change without notice.***

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2