WE HAVE CONTACT LANDS (GOLD PLATED BRASS) SOLDERED ON A PCB. AND THEY HAVE A MATE WITH RECIPROCAL SPRING CONTACTS AS A POWER SWITCH.
WE NEED TO ELEVATE THE CONTACT LANDS TO DECREASE THE CONTACT RESISTANCE. SO WE USED A RING (SILVER PLATED) BETWEEN THE PCB AND CONTACT LAND (GOLD PLATED) BEFORE SOLDERING THEM. DOES THIS SITUATION CAUSE ANY PROBLEM ?
I THINK WE CAN'T USE ANY PLASTIC RING BECAUSE OF THE SPRING PRESSURE (FROM THE OPPOSITE PART) AND THE SOLDERING CONSTRAINTS.
THANK YOU FOR YOUR HELP INGEMAR..
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ingemar Hernefjord
Sent: Tuesday, November 29, 2005 12:30 PM
To: [log in to unmask]
Subject: [TN] SV: [TN] Soldering gold and silver together
Jewellers have joined gold and silver together back to keltic practice,
so it works nice as a gem, but you have to do with connectors, i.e.
current and voltage and maybe even humidity and heat. Using tin, you
will get some intermetallics and maybe brittle joints. When you
connect/disconnect the parts there may be some uncalculated forces.
Manipulating connectors is a dubious thing, depending on what pins you
are talking about: subminiature? Signal? Power? I think most of us would
like to see a photo and some more technical information. Ask Steve to
put a pic on the wall before you go on.
Why do you need a metallic ring? Can't you use some 'plastic' distance
rings?
Inge
-----Ursprungligt meddelande-----
Från: TechNet [mailto:[log in to unmask]] För TUGMEN UNSAL (MIKES INTERNET)
Skickat: den 29 november 2005 10:52
Till: [log in to unmask]
Ämne: [TN] Soldering gold and silver together
Dear all,
We put silver plated ring on the connectors pin to be able to lift up
connectors from PCB. Connector pins are gold plated.
Is it possible to solder (tin) a gold plated and a silver plated
material together ? Two of them can be soldered individually, but can
they be soldered together using tin ?
Any problems we may face to kd
Thank you.
Tugmen.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|