TECHNET Archives

November 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain; charset="iso-8859-1"
Sender:
Subject:
From:
Leo Higgins <[log in to unmask]>
Date:
Mon, 28 Nov 2005 12:06:14 -0800
MIME-Version:
1.0
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Jeff Brown <[log in to unmask]>
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Leo Higgins <[log in to unmask]>
Parts/Attachments:
text/plain (213 lines)
Hi Jeff,
     Printing paste in a grid is the common approach for surface mounting of
large QFNs, but a large QFN is typically only about 10-11 mm sq.  With
surface mounting of packages similar to a QFN, called a thin array plastic
package (TAPP), the body sizes we have run have been as large as 15x15mm and
the paste grid has been the approach used.  The key issue is not to have too
much solder on the PCB pad ("thermal pad") that is opposed to the
package/substrate pad, or it is possible that the small contact pads will
not solder to the boards (solder pool height on the grid vs. on the contact
pads; final solder thickness).  The surface tension of the molten solder
grid should allow the tops of the first pools to melt to allow the solder to
spread across the pad on the bottom of the substrate while the grid pools
spread into the areas not printed on the PCB, pulling the substrate down to
towards the PCB.  Since the outer contact pads are likely to melt first, as
you note, the solder pool heights and resulting thicknesses need to be
balanced somewhat so that the molten solder on the PCB does not float the
substrate and break the solder connections on the few contact pads.  If too
little solder is put on the thermal pad, spreading across the substrate pad
and the thermal pad can cause the solder on the few contact pads to squeeze
out and short to the thermal pad/substrate pad, although a 0.5mm gap is
reasonably "large".
     In the design guides of some companies, and in some published work, it
is shown that approx 50% void area in the solder connection between the
substrate pad and the PCB thermal pad is allowed with little or no negative
impact to thermal sinking into the PCB or electrical resistivity between the
PCB thermal pad and the substrate pad.  So, as long as the joint achieve
this and there are not shorts or opens, you may be good to go.  It may take
a few stencil design iterations to achieve the optimized results.  Some
folks have evaluated a fairly elegant starburst patterns of grids with
smaller openings towards the center and aperture increasing in size as you
move radially from the center out.  Some grid designs print no past in the
center of the pad to allow paste spreading inward and outward.  A slower
ramp in reflow may help as well.


Best regards,
Leo

Leo M. Higgins III, Ph.D.
Vice President Technical Support Operations
ASAT, Inc.
3755 Capital of Texas Highway, Suite 100
Austin, Texas     78704

ph     512-383-4593
fx      512-383-1590
[log in to unmask]
www.asat.com


The information contained in this electronic message is CUSTOMER/SUPPLIER
PRIVILEGED AND CONFIDENTIAL INFORMATION intended only for the use of the
individual or entity named above. If the reader of this message is not the
intended recipient, you are hereby notified that any dissemination,
distribution and copying of this communication is strictly prohibited. If
you have received this communication in error, please immediately notify the
sender by electronic mail. Thank you.



-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Jeff Brown
Sent: Wednesday, November 23, 2005 11:39 PM
To: [log in to unmask]
Subject: Re: [TN] Unusual soldering challenge


Hi Zil,

Unfortunately it's too late to revise the board this time, but I will
pass your suggestion on for next time.

Many thanks,
Jeff

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Zilber Gil
Sent: Wednesday, 23 November 2005 11:01 PM
To: [log in to unmask]
Subject: Re: [TN] Unusual soldering challenge

Hello Jeff,

We had similar components short time ago, and we create a grid in the
aperture of the stencil, similar to what Ivan suggested. The reflow pass
well, but after examine the component with X-ray we saw air trapped in
the solder (about 20% of the area). Thus, I suggest designing the pad on
the PCB the same way as the grid in the stencil.

Regards,

Gil Zilber
Technologist, Elta system Ltd.
Tel. +972-8-8577240
Mobile +972-54-4983222
http://www.iai.co.il/site/en/iai.asp?pi=17887


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Jeff Brown
Sent: Tuesday, November 22, 2005 7:46 AM
To: [log in to unmask]
Subject: [TN] Unusual soldering challenge

Hi Everyone,

We have a problem with a fairly unique component that requires soldering
to a PCB. I'm really hoping that someone has seen this before as it
looking really awkward.

The component is mounted on a piece of fiberglass about 25mm x 16mm. The
footprint consists of a ground pad which takes up 95% of the area, and
four signal pads with 0.5mm clearance from the ground pad.

The manufacturer recommends a grid of stenciled paste for the ground pad
due to the large area, but we are concerned that if the paste melts from
the outside edges in, then it will at a minimum result in flux
entrapment, and at worst, the trapped flux will boil and lift the
component, or move the molten solder causing shorts to the signal pads.

I imagine that even if we used solid paste pattern that this would
probably only make the problem worse.

Or are we just being overly pessimistic?

Any thoughts on options would be gratefully received...  Currently
wondering about the possibility of applying BGA balls to the package so
that there is some clearance between the board and the component.

If anyone is interested, I can send the component datasheet to them
directly.

Thank you all in advance

Jeff Brown and Josh Vear
EOS Space Systems

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------


This message is processed by the PrivaWall Email Security Server.





 The information contained in this communication is proprietary to
Israel Aircraft Industries Ltd.
and/or third parties, may contain confidential or privileged
information, and is intended only for
the use of the intended addressee thereof. If you are not the intended
addressee, please be aware
that any use, disclosure, distribution and/or copying of this
communication is strictly prohibited.
If you receive this communication in error, please notify the sender
immediately and delete it from
your computer. Thank you.


This message is processed by the PrivaWall Email Security Server.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2