TECHNET Archives

November 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 23 Nov 2005 17:20:20 EST
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="US-ASCII"
From:
Werner Engelmaier <[log in to unmask]>
Parts/Attachments:
text/plain (21 lines)
Hi Joel,
If all SnPb solder joints reach 205C thay all will be fine. The problem is
that in most assemblies the differences in T are quite large, and if some SJs
only reach 217C their proper metallurgical bond is not a sure thing. I do not
know what you imply with "he majority of the solder joints on the balance of the
board are getting too hot?" There are no negative consequences to this--I am
much more concern ed about PCBs and components getting too hot. That is where
I see most of the problems with LF-soldering.

Werner

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2