as long as you have sufficient time above liquidus temperature... without
damage your most sensitive parts (like some of the sub-micron devices only
allow 10 -15 sec above 200 C)...this is only apply to reflow oven... not
RTP...No open flame turkey ;-) on thanks giving...
jk
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Joel Mearig
Sent: Wednesday, November 23, 2005 12:37 PM
To: [log in to unmask]
Subject: Re: [TN] Lead Free BGAs
The article indicates that a typical Sn/Pb profile peaks at 220degC. I don't
think anyone should be running Sn/Pb that hot. You don't need to be 40degC
above reflow to form a reliable solder joint. I think a Sn/Pb profile should
max at 205degC.
I wonder if the experimental results would change if he ran a cooler (and in
my opinion more appropriate) profile.
Joel Mearig
Delta Tau Data Systems, Inc.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Dehoyos, Ramon
Sent: Wednesday, November 23, 2005 7:07 AM
To: [log in to unmask]
Subject: [TN] Lead Free BGAs
> Tin/Silver BGAs balls forces oven profiles to be increased so
> that the ball collapses and creates a good SJ when using tin/lead
> solder, according to this article.
> Regards,
> Ramon
>
>
> http://www.empf.org/empfasis/jan05/help0105.htm
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|