Hi richard,
No, this is not an 'Unicum' process, but it is how BGAs were developed. When
larger LLCCCs [for those of you too young--leadless ceramic chip carriers]
could not be used because of premature
SJ failures, we removed the sidewall metallisations at the castellations
[thus eliminating the solder fillets] which allowed the LLCCCs to swim up. When
this proved to be insufficient for SJ reliability, we used solder balls and cast
tin columns [the first BGAs and components with solder (tin) columns--Bell
Labs has a couple of patents on this].
You put the solder balls onto the component by a reflow process [same as a
BGA--it is the high-temperature hand soldering that is the problem with these
components] and you unsolder the components by touching the PCB pad and the
high-melt solder ball, not the component.
Werner
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|