Hi Steve - Yes, I am currently at our Bellevue IA facility (and its snowing
here!) but when I get back to my desk I'll send two photos showing
possible "non-uniform" solder joint microstructure of a SAC405 solderball
in a SnPb soldering process.
Dave
Stephen Gregory
<Stephen.Gregory@
LABARGE.COM> To
Sent by: TechNet [log in to unmask]
<[log in to unmask]> cc
Subject
11/16/2005 02:09 Re: [TN] [LF] Reliability
PM prediction of LF soldering
Please respond to
TechNet E-Mail
Forum
<[log in to unmask]>
; Please respond
to
Stephen Gregory
<Stephen.Gregory@
LABARGE.COM>
Dave,
Can we see it? I'll post it...
-Steve Gregory-
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David D. Hillman
Sent: Wednesday, November 16, 2005 2:03 PM
To: [log in to unmask]
Subject: Re: [TN] [LF] Reliability prediction of LF soldering
Hi Werner! FYI - The "Pbfree BGA gone bad" was shown at the CMAP
conference
in Toronto (not ECTC).
Dave
Werner Engelmaier
<[log in to unmask]
OM>
To
Sent by: TechNet [log in to unmask]
<[log in to unmask]>
cc
Subject
11/16/2005 01:11 Re: [TN] [LF] Reliability
PM prediction of LF soldering
Please respond to
TechNet E-Mail
Forum
<[log in to unmask]>
; Please respond
to
[log in to unmask]
M
Hi Ingemar,
Is this picture similar to the one Dave Hillman showed at ECTC?
Werner
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|