TECHNET Archives

November 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0 (Apple Message framework v746.2)
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Kane, Joseph E (US SSA)" <[log in to unmask]>
Date:
Mon, 14 Nov 2005 12:42:19 -0700
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, David Douthit <[log in to unmask]>
Subject:
From:
David Douthit <[log in to unmask]>
In-Reply-To:
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=US-ASCII; delsp=yes; format=flowed
Parts/Attachments:
text/plain (108 lines)
Joe,

Are you tinning the pins?00 These type of connectors have a fair
amount of metal acting as a heat sink. Tinning the pins prior to
assembly will solve your problem.

David Douthit
Manager
LoCan


On Nov 14, 2005, at 11:15 AM, Kane, Joseph E (US SSA) wrote:

> MIL-C-38999 covers the round connectors that stick out
> of the front of our boxes and let them communicate with
> the airplane.  The outer metal shells are olive drab iridite
> over cad plate, and they mate together with a twist/lock
> collar.
>
> When the suspect solder joint was touched with an iron and some
> Soder Wick, the whole thing disappeared.  There appeared to
> be good wetting to the lead and the pad, but very little
> flow up into the barrel.  Sorry, I don't have a picture.
>
> -Joe
>
> -----Original Message-----
> From: [log in to unmask] [mailto:[log in to unmask]]
> Sent: Monday, November 14, 2005 12:46 PM
> To: [log in to unmask]; Kane, Joseph E (US SSA)
> Subject: RE: [TN] Agilent 5DX Service
>
>
> I am not familiar with the P/N 38999 connector yet you speak of a
> spacer
> which stirs the mind.   Can you share a photo of the animal you are
> talking about and the spacer application with vertical fill anomaly.
>
> Victor,
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Kane, Joseph E (US
> SSA)
> Sent: Monday, November 14, 2005 10:47 AM
> To: [log in to unmask]
> Subject: [TN] Agilent 5DX Service
>
> One of our boards has a number of 38999 connectors, with
> connections on
> the top side hidden by a spacer.  We've had one SJ failure because
> of inadequate solder fill up through the PTH.  We'd like to determine
> whether this is an isolated problem, or whether the spacer might be
> impeding solder flow.  Of course, we don't have any boards to
> sacrifice,
> and we can't see anything with direct transmission x-ray because the
> connector is in the way.
>
> Anyone know of a lab somewhere nearby that offers scan beam
> laminography service?
>
> Joe Kane
> BAE Systems
> Johnson City, NY
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
> unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily
> halt or
> (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
> information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100
> ext.2815
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following
> text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail
> to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/
> archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?
> Pageid=4.3.16 for additional information, or contact Keach Sasamori
> at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2