The NiPdAu lead finish is widely shown by IC makers as the 2nd choice for a
leadfree package finish, with matte tin being number one, even though the
debate about whiskering with tin continues unabated. Some companies have
made NiPdAu their first choice for packages with long leads where leadfree
SMT solder will not coat the total lead length during reflow. In general,
requests for qualification of IC components with the NiPdAu finish is
increasing, so it is likely that its use will continue to grow and become
more common as we approach July 2006.
Best regards,
Leo
Leo M. Higgins III, Ph.D.
Vice President Technical Support Operations
ASAT, Inc.
3755 Capital of Texas Highway, Suite 100
Austin, Texas 78704
ph 512-383-4593
fx 512-383-1590
[log in to unmask]
www.asat.com
The information contained in this electronic message is CUSTOMER/SUPPLIER
PRIVILEGED AND CONFIDENTIAL INFORMATION intended only for the use of the
individual or entity named above. If the reader of this message is not the
intended recipient, you are hereby notified that any dissemination,
distribution and copying of this communication is strictly prohibited. If
you have received this communication in error, please immediately notify the
sender by electronic mail. Thank you.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Stadem, Richard
Sent: Monday, November 14, 2005 6:55 AM
To: [log in to unmask]
Subject: Re: [TN] IC's with NiPdAu finish
TI has done this for many years. I have run into some issues with it at
different companies. I do not know if other component companies are also
using it as a terminal finish, but I suspect so.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David Greig
Sent: Sunday, November 13, 2005 10:46 AM
To: [log in to unmask]
Subject: [TN] IC's with NiPdAu finish
Hi TN,
Just noticed that TI are using this finish for a great many leadframe
packages (QFP, TSSOP etc).
Is this finish becoming widespread in the industry?
Best Regards
David Greig
______________________________
GigaDyne Ltd
Buchan House
Carnegie Campus
Dunfermline KY11 8PL
United Kingdom
t: +44 (0)1383 624 975
www.gigadyne.co.uk <http://www.gigadyne.co.uk/>
______________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|