TECHNET Archives

November 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Mon, 14 Nov 2005 10:03:45 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Richard Kraszewski <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
Richard Kraszewski <[log in to unmask]>
Parts/Attachments:
text/plain (34 lines)
While I know that the nominal value would be dependent on many factors
such as paste product, print speed, pad sizes, blade material etc., I'm
trying to determine what would be a typical and realistic volume range
that one might expect to get on printed paste deposits.    When you
really look at the details presented by a rather large and well-know
paste inspection equipment manufacturer, they indicate that +/- 17% is
not unusual even in laboratory type environments. 

 

Just curious as to what some practical experiences out there might be.

 

Seems to be an area with a lot of assumptions that these instruments
provide more discriminating information that they actually do. 

 

Rich K/ KEDS

 


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2