TECHNET Archives

November 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0 (Apple Message framework v746.2)
Sender:
X-To:
[log in to unmask], TechNet E-Mail Forum <[log in to unmask]>
Date:
Fri, 11 Nov 2005 12:18:54 +0100
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Ivanoe Pedruzzi <[log in to unmask]>
Subject:
From:
Ivanoe Pedruzzi <[log in to unmask]>
In-Reply-To:
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=US-ASCII; delsp=yes; format=flowed
Parts/Attachments:
text/plain (149 lines)
Mike,
why do you advice not to mix used paste with fresh one? What someone
can expect to happen,  from a reflow and soldering point of view?

(please consider that we are talking about used paste I woudn't think
to have more than 20% in  volume to mix on a stencil and also I
wouldn't go for mixing it in only one time, so it gets diluted over a
working shift)

THX, Ivan


Il giorno 11/nov/05, alle ore 12:01, Mike Fenner ha scritto:

> The answer is really you can't tell by testing. Even if you
> duplicated a
> solder paste QA lab on your shop floor, you could test the paste
> and find it
> OK, but still not know how much of its life had been used compared
> to new.
> The best thing to do is to control the rate of issue of paste to
> the shop
> floor and put in place some rules on re-use of paste to make an SOP
> for
> operator. Then for your ISO guy demonstrate you follow the SOP.
> Eg
> Only issue what is used in a shift (commensurate with loading stencil)
> Used paste goes in jars marked used paste. Never mix it with new
> paste.
> Use only new paste to load stencil.
> Old paste is only used to replenish stencil (if you are concerned
> to re-use
> paste)
> Discard used paste after x day
> Also put in some best practice rules: Keep jars closed when not in use
> And so on.
> The precise rate of discard etc can be set arbitrarily or by
> reference to
> your fault rates. [Would give your ISO guy something to do :)
>
> Finally whilst no one condones unnecessary waste, don't forget the
> object is
> to produce products not save paste. Solder costs are a tiny part of
> your
> overall spend, you can't really save a huge amount of money on
> solder, but
> you can easily incur costs with non spec materials. That is the
> real benefit
> of the SOP.
>
> Regards
>
> Mike Fenner
> Indium Corporation
> Pb-free at Productronica
> www.indium.com/productronica/
>
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Yannick Brisson
> Sent: 10 November 2005 19:57
> To: [log in to unmask]
> Subject: [TN] Solder paste control
>
> Hi,
>
>         I had a question from our ISO guy asking me how I know that
> the
> paste we use is in good condition?  The problem is that he saw our
> operator
> put some old paste back in a empty jar to reuse it the next day. So
> his
> question is how do you know the paste has been on the stencil below
> the
> maximal hour wrote in the datasheet?  Do you know any measure than
> I can
> take to certify that the paste in good? like viscosity or something
> else?
> And how I do that?  Because I'm pretty sure that is next question
> will be
> how I know the new paste we just receive is good too.
>
> Thank You
>
> Yannick
>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
> unsubscribe, send a message to [log in to unmask] with following text
> in the
> BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
> (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
> Technet
> NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
> e-mail to [log in to unmask]: SET Technet Digest Search the archives of
> previous posts at: http://listserv.ipc.org/archives Please visit
> IPC web
> site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
> information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100
> ext.2815
> -----------------------------------------------------
>
>
> ***This email, its content and any files transmitted with it are
> intended solely for the addressee(s) and may be legally privileged
> and/or confidential. If you are not the intended recipient please
> delete and contact the sender by return and delete the material
> from any computer. Any review, retransmission, dissemination or
> other use of, or taking of any action in reliance upon, this
> information by persons or entities other than the intended
> recipient is prohibited.
>
> Messages sent via this medium may be subject to delays, non-
> delivery and unauthorized alteration. This email has been prepared
> using information believed by the author to be reliable and
> accurate, but Indium Corporation makes no warranty as to accuracy
> or completeness. In particular, Indium Corporation does not accept
> responsibility for changes made to this email after it was sent.
> Any opinions or recommendations expressed herein are solely those
> of the author. They may be subject to change without notice.***
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following
> text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail
> to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/
> archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?
> Pageid=4.3.16 for additional information, or contact Keach Sasamori
> at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2