You can HASL with any solder suitable for electronics. In general the
surface smoothness should be the same if done correctly. A tighter range is
possible with most lead free alloys.
-----Original Message-----
From: Babcock John [mailto:[log in to unmask]]
Sent: 10 November 2005 09:09 PM
To: [log in to unmask]
Subject: [TN] plating smoothness
Does anybody call out a specific smoothness finish ever on a fabrication dwg
for the HASL? In these days of lead free, going forawrd, I am wondering if
silver will have the same smoothness finish as SN63/PB37 using HASL?
1) Or can you HASL with silver?
2) Does anyone have an example of a fab note for such a callout? Or is
this getting too specific?
John Babcock
PCB Designer III
Isothermal Systems Research (ISR)
2218 N. Molter Rd
Liberty Lake, WA 99019
[log in to unmask]
P: (509) 241-4641
F: (509) 444-1082
This E-mail and any files transmitted with it are confidential and
proprietary in nature and intended solely for the use of the individual to
whom it is addressed. If you have received this E-mail in error, please
send it back to the person that sent it to you. Any views or opinions
presented are solely those of its author and do not necessarily
represent those of Isothermal Systems Research, Inc. Unauthorized
publication, use, dissemination, forwarding, printing or copying of this
email and its associated attachments is strictly prohibited. Thank you for
your cooperation.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|