TECHNET Archives

November 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Wee Mei <[log in to unmask]>
Date:
Thu, 10 Nov 2005 08:53:14 -0500
Reply-To:
Content-Transfer-Encoding:
7bit
Subject:
From:
Kevin Glidden <[log in to unmask]>
Content-Type:
text/plain; charset="us-ascii"
In-Reply-To:
Organization:
LSI
MIME-Version:
1.0
Parts/Attachments:
text/plain (193 lines)
There are multiple MIL specs governing connectors.  The most common is
MIL-A-28870 "Assemblies, Electrical Backplane, Printed-Wiring, General
Specification For", which is widely (and often incorrectly) referenced.
This specification does give criteria for press fit pins, but only for those
that are per MIL-C-28859 requirements.  Not all connectors are MIL-C-28859
compliant.

IEC also maintains specifications for numerous connector styles.

Again, check the technical literature from the connector manufacturer of the
connector you are using.  Even if the connector is not certified to some
industry specification, they should be able to give you performance data.



-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Wee Mei
Sent: Thursday, November 10, 2005 4:15 AM
To: [log in to unmask]
Subject: Re: [TN] Press-fit pins and polyimide laminate

Hello,

I remember there is a standard that governs press-fit connector. Is it MIL
or IPC? My memory suddenly failed me totally.

Regards,
Wee Mei

----- Original Message -----
From: "Wee Mei" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Thursday, November 10, 2005 11:23 AM
Subject: Re: [TN] Press-fit pins and polyimide laminate


> Hello,
>
> I would like to join in to ask some questions about press-fit
> connectors on flex circuit :
>
> 1. Can press fit connector be used on flex circuit? My opinion is no
> unless it is on the rigid section. But then how about MLB flex? How
> many layers then is good for press-fit.
>
> 2. Does the rules for press-fit on rigid board apply to mulitlayer
> flex too?
>
> 3. Must press-fit connector be assemblied using a tool or can they be
> pushed in by hands?
>
> Regards,
> Wee Mei
>
> ----- Original Message -----
> From: "Zilber Gil" <[log in to unmask]>
> To: <[log in to unmask]>
> Sent: Wednesday, November 09, 2005 2:37 AM
> Subject: Re: [TN] Press-fit pins and polyimide laminate
>
>
>> We are using press fit in polyimide laminates for many years without
>> any problem. They pass all the military reliability test. A good
>> support of the boar during the assembly is important.
>>
>> Regards,
>>
>> Dr. Gil Zilber
>> Technologist, Elta system Ltd.
>> Tel. +972-8-8577240
>> Mobile +972-54-4983222
>> http://www.iai.co.il/site/en/iai.asp?pi=17887
>>
>>
>>
>> -----Original Message-----
>> From: TechNet [mailto:[log in to unmask]] On Behalf Of Geoff Layhe of
>> Lamar Group
>> Sent: Tuesday, November 08, 2005 7:29 PM
>> To: [log in to unmask]
>> Subject: [TN] Press-fit pins and polyimide laminate
>>
>> Does anybody have information about the suitability of polyimide (or
>> any other high temp laminate) with press fit pins.
>>
>> It doesn't seem a good idea to me to use them with poyimide being
>> more brittle than FR4 but are there any guidelines anywhere?
>>
>> Geoff Layhe
>>
>> Private & Confidential:
>>
>> This e-mail message is confidential and is intended solely for the
>> person or organisation to whom it is addressed.  If the message is
>> received by anyone other than the addressee please return the message
>> to the sender by replying to it and then delete the message from your
>> computer.
>>
>>
>>
>>
>>
>> ---------------------------------------------------
>> Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
>> unsubscribe, send a message to [log in to unmask] with following text
>> in the BODY (NOT the subject field): SIGNOFF Technet To temporarily
>> halt or
>> (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
>> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
>> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
>> archives of previous posts at: http://listserv.ipc.org/archives
>> Please visit IPC web site
>> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
>> information, or contact Keach Sasamori at [log in to unmask] or
>> 847-615-7100 ext.2815
>> -----------------------------------------------------
>>
>>
>> This message is processed by the PrivaWall Email Security Server.
>>
>>
>>
>>
>>
>> The information contained in this communication is proprietary to
>> Israel Aircraft Industries Ltd.
>> and/or third parties, may contain confidential or privileged
>> information, and is intended only for the use of the intended
>> addressee thereof. If you are not the intended addressee, please be
>> aware that any use, disclosure, distribution and/or copying of this
>> communication is strictly prohibited.
>> If you receive this communication in error, please notify the sender
>> immediately and delete it from your computer. Thank you.
>>
>>
>> This message is processed by the PrivaWall Email Security Server.
>>
>> ---------------------------------------------------
>> Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
>> unsubscribe, send a message to [log in to unmask] with following text
>> in the BODY (NOT the subject field): SIGNOFF Technet To temporarily
>> halt or (re-start) delivery of Technet send e-mail to
>> [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
>> per day of all the posts: send e-mail to
>> [log in to unmask]: SET Technet Digest
>> Search the archives of previous posts at:
>> http://listserv.ipc.org/archives
>> Please visit IPC web site
>> http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>> for additional information, or contact Keach Sasamori at
>> [log in to unmask] or 847-615-7100 ext.2815
>> -----------------------------------------------------
>>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
> unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
> or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
> per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at
> [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2