John,
We thermal cycle at similar conditions (typical for us is -55 / +70 c) but
I've done some testing at -65/ +100. You should, in my opinion, expect good
results. (ie no plating cracks).
Worst case scenerio - Thick board, non functional pads removed, FR4
material. With this set up you'll see a lot of Z axis
expansion/contraction. If the plated copper is robust you will have a
better chance of survival. If you have less robust copper you will have
failures. Other criteria is important - hole size, Tg of material and
more...
Two fixes come to mind. Work with the board fabricator. If they can improve
there plating that may be all that is necessary. Or internally you could
have your designers add the non functional pads back into the board....
good luck
Pete
>From: Babcock John <[log in to unmask]>
>Reply-To: TechNet E-Mail Forum <[log in to unmask]>, Babcock John
><[log in to unmask]>
>To: [log in to unmask]
>Subject: [TN] Temperature Cycling
>Date: Mon, 7 Nov 2005 16:29:08 -0800
>
>Does anybody know of any special considerations on circuit boards for
>temperature cycling. We are testing the board to -65C to +85C. We are
>seeing via barrels cracking and TH connector solder joints cracking. Do
>we need to add extra pad area? Just curious if there is an IPC document
>on cold temperatures or temp. cycling and causing stress on the circuit
>boards.
>
>Thanks!
>
>John Babcock
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>for additional information, or contact Keach Sasamori at [log in to unmask] or
>847-615-7100 ext.2815
>-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|