We are using press fit in polyimide laminates for many years without
any problem. They pass all the military reliability test. A good support
of the boar during the assembly is important.
Regards,
Dr. Gil Zilber
Technologist, Elta system Ltd.
Tel. +972-8-8577240
Mobile +972-54-4983222
http://www.iai.co.il/site/en/iai.asp?pi=17887
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Geoff Layhe of Lamar
Group
Sent: Tuesday, November 08, 2005 7:29 PM
To: [log in to unmask]
Subject: [TN] Press-fit pins and polyimide laminate
Does anybody have information about the suitability of polyimide (or any
other high temp laminate) with press fit pins.
It doesn't seem a good idea to me to use them with poyimide being more
brittle than FR4 but are there any guidelines anywhere?
Geoff Layhe
Private & Confidential:
This e-mail message is confidential and is intended solely for the
person or organisation to whom it is addressed. If the message is
received by anyone other than the addressee please return the message to
the sender by replying to it and then delete the message from your
computer.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
This message is processed by the PrivaWall Email Security Server.
The information contained in this communication is proprietary to Israel Aircraft Industries Ltd.
and/or third parties, may contain confidential or privileged information, and is intended only for
the use of the intended addressee thereof. If you are not the intended addressee, please be aware
that any use, disclosure, distribution and/or copying of this communication is strictly prohibited.
If you receive this communication in error, please notify the sender immediately and delete it from
your computer. Thank you.
This message is processed by the PrivaWall Email Security Server.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|