TECHNET Archives

November 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Hans Shin <[log in to unmask]>
Date:
Tue, 1 Nov 2005 11:04:12 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Stadem, Richard" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
"Stadem, Richard" <[log in to unmask]>
Parts/Attachments:
text/plain (65 lines)
Another way is to remove a small amount of solder from different solder
joints and send it to one of the solder analysis companies, just as you
would a solder sample from a wave solder pot. It may not be as accurate
as some of the other methods, but it will certainly be a low cost method
that would give you a pretty good indication. 

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Hans Shin
Sent: Tuesday, November 01, 2005 10:41 AM
To: [log in to unmask]
Subject: Re: [TN] Lead-Free testing

Carl,

To answer both of your questions, SEM/EDS analysis is a good way to see
if it's a Pb-free solder or Sn/Pb solder.  If you have XRF with
elemental characterization capability, that should work as well.  The
instrument chambers should accomodate most sizes.  If not, a tiny amount
of solder can be removed from one location for SEM/EDS analysis.

Hans Shin
Pacific Testing Laboratories, Inc.
www.pacifictesting.com


-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Carl VanWormer
Sent: Tuesday, November 01, 2005 8:27 AM
To: [log in to unmask]
Subject: [TN] Lead-Free testing


Is there an easy way to verify that an assembly has been produced with
lead-free solder?  Conversely, is there a quick and easy test for lead
in a solder joint?

Carl Van Wormer
Cipher Systems
1800 NW 169th Place, Suite B-100
Beaverton, OR  97006
Phone (503)-617-7447    Fax (503)-617-6550

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest