Joel:
Understood.....if the part won't take the heat...it limits your options.
I like Rainer Blomberg's process option. Perhaps that would work?
On Tue, 4 Oct 2005 09:56:07 -0700, Joel Mearig <[log in to unmask]> wrote:
>Kelly,
>Thanks for the input.
>
>First, I forgot to mention that I am in a lead-free process and the plastic
>of the connectors will not stand-up to the higher reflow temperatures.
>
>Second, the flux application would have to be very controlled because the
>solder would tend to chase up the lead if the flux did the same thing due
to
>the solderability of the Gold. I haven't tried performs so maybe I am
>creating a problem, in my mind, that doesn't exist in application.
>Joel
>
>-----Original Message-----
>From: TechNet [mailto:[log in to unmask]] On Behalf Of Kelly Morris
>Sent: Tuesday, October 04, 2005 9:36 AM
>To: [log in to unmask]
>Subject: Re: [TN] Hand Soldering Long Gold Pins
>
>On Tue, 4 Oct 2005 09:41:57 -0700, Joel Mearig <[log in to unmask]>
wrote:
>
>>Kelly,
>>The pins are part of a connector so they are solid from that view points.
>>They are not tight in the thru-holes so they must be tacked to secure
>before
>>soldering balance of pins. Joel
>>
>>-----Original Message-----
>>From: TechNet [mailto:[log in to unmask]] On Behalf Of Kelly Morris
>>Sent: Tuesday, October 04, 2005 9:17 AM
>>To: [log in to unmask]
>>Subject: Re: [TN] Hand Soldering Long Gold Pins
>>
>>Joel:
>>Are the pins you are trying to solder secure in the thru-holes before
>>soldering, or are they loose?
>>
>>---------------------------------------------------
>>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>>To unsubscribe, send a message to [log in to unmask] with following text in
>>the BODY (NOT the subject field): SIGNOFF Technet
>>To temporarily halt or (re-start) delivery of Technet send e-mail to
>>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>>To receive ONE mailing per day of all the posts: send e-mail to
>>[log in to unmask]: SET Technet Digest
>>Search the archives of previous posts at: http://listserv.ipc.org/archives
>>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>>for additional information, or contact Keach Sasamori at [log in to unmask] or
>>847-615-7100 ext.2815
>>-----------------------------------------------------
>>
>>---------------------------------------------------
>>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>>To unsubscribe, send a message to [log in to unmask] with following text in
>>the BODY (NOT the subject field): SIGNOFF Technet
>>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>>Search the archives of previous posts at: http://listserv.ipc.org/archives
>>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>for additional information, or contact Keach Sasamori at [log in to unmask] or
>847-615-7100 ext.2815
>>-----------------------------------------------------
>
>Joel:
>I beleive these connectors are available with solder bearing leads. Then
>all you have to do is add flux and send through a reflow oven.
>
>If you must deal with the connectors you have, you might want to consider
>solder preforms. They should be available from your solder/flux supplier.
>Then all you do is slip a solder preform (shaped like a washer) over each
>pin and add flux (if its not already on the preform) and then send thru
>your reflow oven.
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>for additional information, or contact Keach Sasamori at [log in to unmask] or
>847-615-7100 ext.2815
>-----------------------------------------------------
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
>-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|