TECHNET Archives

October 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Geoff Layhe of Lamar Group <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Geoff Layhe of Lamar Group <[log in to unmask]>
Date:
Fri, 14 Oct 2005 16:22:12 +0100
Content-Type:
text/plain
Parts/Attachments:
text/plain (57 lines)
I think this was mil spec for unclad material
I got the following from:-
http://store.ihs.com/specsstore/controller;jsessionid=SlnzJfSmElCg5PSxvJQ0TA**.app1?event=PROCESS_COUNTRY&originEvent=SEARCH_RESULTS

looks like its cancelled.

NAVY  MIL-P-18177C CANC NOTICE 1
1992-FEB-25   * Cancelled * 
PLASTIC SHEET, LAMINATED, THERMOSETTING, GLASS, FIBER BASE, EPOXY-RESIN  

Geoff Layhe

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of John Parsons
Sent: Friday, October 14, 2005 3:59 PM
To: [log in to unmask]
Subject: [TN] MIL-P-18177


Good morning all,

I have a customer spec'ing a PCB from laminate meeting MIL-P-18177/GEE.  I
can't seem to find a copy of the MIL-P-18177 spec but an internet search
turns up reference to this spec and FR-4/G10 materials.  None of my material
spec sheets make reference however.  Can anyone shed some light on this
requirement.

TIA

John Parsons

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

Private & Confidential:

This e-mail message is confidential and is intended solely for the person or organisation to whom it is addressed.  If the message is received by anyone other than the addressee please return the message to the sender by replying to it and then delete the message from your computer.

 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2